Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 26 g/10 min @Load 5.00 kg, Temperature 260 °C |
26 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics GELOY XP7550 ASA+PC (Asia Pacific) Injection molding ASA-PC Blend suitable for exterior applications featuring outdoor weatherability, toughness, good heat performance and excellent flow. |
|||
Melt Index of Compound | 26 g/10 min @Load 1.20 kg, Temperature 300 °C |
26 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® FXD173R PC (Europe-Africa-Middle East) LEXAN FXD173R is a UV stabilized translucent high flow grade for light diffusion special effects. The color package may affect performance. |
|||
Melt Index of Compound | 26 g/10 min @Load 1.20 kg, Temperature 300 °C |
26 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® FXE171R PC (Europe-Africa-Middle East) LEXAN FXE171R is a transparent/translucent high flow grade for special effects colors with a fluorescent appearance. Color package may affect performance. |
|||
Melt Index of Compound | 26 g/10 min @Load 1.20 kg, Temperature 300 °C |
26 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® FXM171R PC (Europe-Africa-Middle East) LEXAN FXM171R is a transparent/translucent high flow grade for special effects colors with a metallic-luster appearance. Color package may affect performance. |
|||
Melt Index of Compound | 26 g/10 min @Load 1.20 kg, Temperature 300 °C |
26 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HF1110 PC (Europe-Africa-Middle East) LEXAN HF1110 is a high flow grade especially designed for applications that require thin wall sections and high flow lengths. |
|||
Melt Index of Compound | 26 g/10 min @Load 1.20 kg, Temperature 300 °C |
26 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HF1110R PC (Europe-Africa-Middle East) LEXAN HF1110R is a high flow grade especially designed for applications that require thin wall sections and high flow lengths. |
|||
Melt Index of Compound | 26 g/10 min @Load 1.20 kg, Temperature 300 °C |
26 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HF1130R PC (Europe-Africa-Middle East) LEXAN HF1130R is a high flow, UV stabilized, grade especially designed for applications that require thin wall sections and higher flow lengths. |
|||
Melt Index of Compound | 26 g/10 min @Load 1.20 kg, Temperature 300 °C |
26 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HF1140R PC (Europe-Africa-Middle East) LEXAN HF1140R is a high flow grade. This material is especially designed for applications that require thin wall sections and high flow lengths. FDA food contact compliant in limited colors.Effect.. |
|||
Melt Index of Compound | 26 g/10 min @Load 1.20 kg, Temperature 300 °C |
26 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HP1NREU PC (Europe-Africa-Middle East) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains no mold release. |
|||
Melt Index of Compound | 26 g/10 min @Load 1.20 kg, Temperature 300 °C |
26 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HP1REU PC (Europe-Africa-Middle East) High flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO sterilizable. Contains mold release. |
|||
Melt Index of Compound | 26 g/10 min @Load 1.20 kg, Temperature 300 °C |
26 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® OQ3120 PC (Europe-Africa-Middle East) High Flow. UV-stabilized. Inherent mold release. Ophthalmic lenses. |
|||
Melt Index of Compound | 26 g/10 min @Load 5.00 kg, Temperature 260 °C |
26 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics GELOY XP7550 ASA+PC Injection molding ASA-PC Blend suitable for exterior applications featuring outdoor weatherability, toughness, good heat performance and excellent flow. |
|||
Melt Index of Compound | 26 g/10 min @Load 5.00 kg, Temperature 260 °C |
26 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics GELOY XP7550 ASA+PC (Europe-Africa-Middle East) Injection molding ASA-PC Blend suitable for exterior applications featuring outdoor weatherability, toughness, good heat performance and excellent flow. |
|||
Melt Index of Compound | 26 g/10 min @Load 1.20 kg, Temperature 300 °C |
26 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® FXD171R PC (Europe-Africa-Middle East) LEXAN FXD171R is a transparent/translucent high flow grade for light diffusion special effects. Color package may affect performance. |
|||
Melt Index of Compound | 26 g/10 min @Load 1.20 kg, Temperature 300 °C |
26 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® HF1140 PC (Europe-Africa-Middle East) Ideal for disposables/short life cycles. Good clarity, heat resistance, property retention and dimensional stability. FDA food contact compliant in limited colors.Effective January 15th, 2007 this.. |
|||
Melt Index of Compound | 26 g/10 min @Load 2.16 kg, Temperature 260 °C |
26 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
Mitsui APELâ„¢ APL6011T Cyclo Olefin Copolymer (COC) This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces.. |
|||
Melt Index of Compound | 26 g/10 min @Load 5.00 kg, Temperature 260 °C |
26 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics LNP LUBRICOMP NL001 PC+ABS LNP LUBRICOMP* NL001 is a compound b ased on PC+ABS resin containing 5% PTFE. Added features include: Wear Resistant, Suitable for Thin Wall Applications. |
|||
Melt Index of Compound | 26 g/10 min @Load 5.00 kg, Temperature 260 °C |
26 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics LNP LUBRICOMP NL001 PC+ABS (Europe-Africa-Middle East) LNP LUBRICOMP* NL001 is a wear resistant PC+ABS blend, suitable for thin wall applications. |
|||
Melt Index of Compound | 26 g/10 min @Load 1.20 kg, Temperature 300 °C |
26 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics PC2800 PC (Europe-Africa-Middle East) PC2800 resin is a high flow (MFR = 28 at 300°C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release... |
|||
Melt Index of Compound | 26 g/10 min @Load 2.16 kg, Temperature 300 °C |
26 g/10 min @Load 4.76 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics LNP STAT-KON DX09315C PC (Asia Pacific) LNP* Stat-Kon* DX09315C is carbon fiber filled polycarbonate composite with good flow ability, and high level of cleanliness for the most demanding application. A unique feature of this material is .. |
|||
Melt Index of Compound | 26 g/10 min @Load 2.16 kg, Temperature 250 °C |
26 g/10 min @Load 4.76 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® K3501 PBT Unfilled PBT, Hydrollytically Stable, Heat Stabilized, Impact Modified. A hydrollytically stable grade designed for improved performance under heat/humidity environments. Targeted at automotive unde.. |
|||
Melt Index of Compound | 26 g/10 min @Load 2.16 kg, Temperature 250 °C |
26 g/10 min @Load 4.76 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® K3501 PBT (Europe-Africa-Middle East) Unfilled PBT, Hydrollytically Stable, Heat Stabilized, Impact Modified. A hydrollytically stable grade designed for improved performance under heat/humidity environments. Targeted at automotive unde.. |
|||
Melt Index of Compound | 26 g/10 min @Load 5.00 kg, Temperature 300 °C |
26 g/10 min @Load 11.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL EXNL0143 PPE+PS Noryl PX1736 Resin is a blend of PPE and PS, that provides high strength, increased heat resistance, and translucency. The material has melt strenght suitable for Extrusion and Blow Molding applica.. |
|||
Melt Index of Compound | 26 g/10 min @Load 5.00 kg, Temperature 300 °C |
26 g/10 min @Load 11.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL PX1736 PPE+PS Noryl PX1736 Resin is a blend of PPE and PS, that provides high strength, increased heat resistance, and translucency. The material has melt strenght suitable for Extrusion and Blow Molding applica.. |