Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 12 g/10 min @Load 5.00 kg, Temperature 260 °C |
12 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Polykemi AB POLYblend 83EFR PC/ABS-Blend, Flame Retardant, Halogen Free Information provided by Polykemi AB |
|||
Melt Index of Compound | 12 g/10 min @Load 2.16 kg, Temperature 230 °C |
12 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYelast TPE R44 TV10 Thermoplastic Elastomer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 12 g/10 min @Load 2.16 kg, Temperature 230 °C |
12 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH GF12030 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Melt Index of Compound | 12 g/10 min @Load 1.20 kg, Temperature 300 °C |
12 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 244R PC 10.5 MFR. Improved flame retardance. USA FDA compliant (limited colors). Internal mold release. |
|||
Melt Index of Compound | 12 g/10 min @Load 1.20 kg, Temperature 300 °C |
12 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 920A PC (Europe-Africa-Middle East) LEXAN 920A is a medium viscosity flame retardant grade, especially suitable for electrical applications. |
|||
Melt Index of Compound | 12 g/10 min @Load 1.20 kg, Temperature 300 °C |
12 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® AD143 PC (Asia Pacific) LEXAN AD143 is a medium viscosity, injection molding grade exhibiting low dust attraction. It is designed for applications with high optical requirements in terms of clarity and light transmission .. |
|||
Melt Index of Compound | 12 g/10 min @Load 1.20 kg, Temperature 300 °C |
12 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® OQ3420 PC (Europe-Africa-Middle East) Medium Viscosity, UV-stabilized grade for ophthalmic lenses. |
|||
Melt Index of Compound | 12 g/10 min @Load 2.16 kg, Temperature 230 °C |
12 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PP EIP12030RF Polypropylene/EPDM, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 12 g/10 min @Load 5.00 kg, Temperature 260 °C |
12 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS (Asia Pacific) Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior... |
|||
Melt Index of Compound | 12 g/10 min @Load 1.20 kg, Temperature 300 °C |
12 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 141R PC (Europe-Africa-Middle East) LEXAN 141R is a medium viscosity multi purpose grade and contains a release agent to ensure easy processing. LEXAN 141R is available in transparent, translucent and opaque colours. |
|||
Melt Index of Compound | 12 g/10 min @Load 1.20 kg, Temperature 300 °C |
12 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 144R PC (Europe-Africa-Middle East) Medium viscosity, multi purpose polycarbonate resin with added release agent. Food contact approved in limited colors. Effective January 15th, 2007 this grade will no longer be supported with bioc.. |
|||
Melt Index of Compound | 12 g/10 min @Load 2.16 kg, Temperature 190 °C |
12 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm3/10 min; ISO 1133 |
DuPont Performance Polymers Delrin® FG500TL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500TL medium viscosity acetal homopolymer resin containing 1.5% Teflon® PTFE Micropowder. It has been developed for consideration into applications such as parts for the food industry.In.. |
|||
Melt Index of Compound | 12 g/10 min @Load 5.00 kg, Temperature 280 °C |
12 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL PX6120 PPE+PS (Asia Pacific) Noryl PX6120 is an unfilled material with good flow, high Impact and chemical resistance against cleaners. Noryl PX6120 is developed for personal care appplications. |
|||
Melt Index of Compound | 12 g/10 min @Load 10.0 kg, Temperature 280 °C |
12 g/10 min @Load 22.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL SE1GFN2 PPE+HIPS (Europe-Africa-Middle East) Noryl* SE1GFN2 is a 20% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non.. |
|||
Melt Index of Compound | 12 g/10 min @Load 5.00 kg, Temperature 340 °C |
12 g/10 min @Load 11.0 lb, Temperature 644 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 1100 PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C). UL94 V0, V2 and 5VA listing. |
|||
Melt Index of Compound | 12 g/10 min @Load 5.00 kg, Temperature 360 °C |
12 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 2310EPR PEI 30% Glass fiber filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Melt Index of Compound | 12 g/10 min @Load 5.00 kg, Temperature 360 °C |
12 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 2312 PEI (Europe-Africa-Middle East) 30% Milled glass filled, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Melt Index of Compound | 12 g/10 min @Load 5.00 kg, Temperature 250 °C |
12 g/10 min @Load 11.0 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Xenoy® IQ1103 PBT+PC Xenoy iQ*1103 resin - Environmentally responsible and sustainable low carbon footprint resin. Xenoy iQ1103 is an unreinforced, impact modified alloy of PC (polycarbonate) + Valox iQ* PBT (polybuty.. |
|||
Melt Index of Compound | 12 g/10 min @Load 5.00 kg, Temperature 250 °C |
12 g/10 min @Load 11.0 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Xenoy® IQ1103U PBT+PC Xenoy* Resin iQ1103U - Environmetally responsible, sustainable, and low carbon footprint resin. Xenoy iQ1103U is an unreinforced, UV stable, impact modified PC+ iQ-PBT alloy with excellent low temp.. |
|||
Melt Index of Compound | 12 - 14 g/10 min | 12 - 14 g/10 min | |
Sibur ABS 2020-30M Molding Grade ABS Plastic With high thermal and light resistance for automobile building, stable to atmospheric conditions in thermal and electric ageing, contacting with food products, as well as with compounding with PC. |
|||
Melt Index of Compound | 12 - 14 g/10 min | 12 - 14 g/10 min | I Preparation |
Sibur ABS 2020-32 Molding Grade ABS Plastic Thermal, light and atmospheric resistant with high fluidity for technical articles and parts of automobile building. |
|||
Melt Index of Compound | 12 g/10 min @Load 5.00 kg, Temperature 280 °C |
12 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Asia Pacific) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Melt Index of Compound | 12 g/10 min @Load 5.00 kg, Temperature 260 °C |
12 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL PPX PPX7112 PPE+PP (Europe-Africa-Middle East) PPE+PP blend. Suitable for painted exterior automotive applications. |
|||
Melt Index of Compound | 12 g/10 min @Load 5.00 kg, Temperature 260 °C |
12 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL PPX PPX7115 PPE+PP High modulus/impact/heat PPE+PP |
|||
Melt Index of Compound | 12 g/10 min @Load 5.00 kg, Temperature 250 °C |
12 g/10 min @Load 11.0 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® V4860HR PBT (Europe-Africa-Middle East) 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified. |
|||
Melt Index of Compound | 12 g/10 min @Load 2.16 kg, Temperature 230 °C |
12 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 2173-01 Polypropylene High-Impact Polypropylene DescriptionPolypropylene PP 2173-01 is a relatively medium flow, high-impact polypropylene for injection molded parts. ApplicationPP 2173-01 meets FDA Regulation 21 CFR 177.1250 for food contact app.. |
|||
Melt Index of Compound | 12 g/10 min @Temperature 230 °C |
12 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 3449-01 Polypropylene Copolymer Polypropylene DescriptionPolypropylene PP 3449-01 is a new generation copolymer polypropylene utilizing unique catalyst technology. Combining an excellent balance of high stiffness and impact. This product inc.. |
|||
Melt Index of Compound | 12 g/10 min @Temperature 230 °C |
12 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 3449-01 Polypropylene Copolymer Polypropylene DescriptionPolypropylene PP 3449-01 is a new generation copolymer polypropylene utilizing unique catalyst technology. Combining an excellent balance of high stiffness and impact. This product inc.. |
|||
Melt Index of Compound | 12 g/10 min | 12 g/10 min | Q-409A-87 (JIS K 7210) |
Zeon Chemicals Quintac® 3451 SIS Rubber |
|||
Melt Index of Compound | 12 g/10 min @Load 1.20 kg, Temperature 300 °C |
12 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® EXL9414T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL9414T resin grade is a halogen-free flame retardant polycarbonate featuring transparency, -40 degree C ductility and UL-94 V0 rating for injection molding applications. Excellent impact co.. |