Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 11.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
11.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ovation Polymers OPTRENE 30GF Polypropylene, 30% Glass Reinforced Properties of chemically coupled glass reinforced (30%) polypropylene with high strength and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All .. |