Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYelast TPE EC12 D55 Thermoplastic Elastomer Information provided by Polykemi AB |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPC T1030 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH GF1020 Polypropylene Homopolymer, Glass Fibre-Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPH T1040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trilene® TS 8058 LLDPE-C6 and LDPE Blend The Trilene TS 8058 product is a blend with a high ratio of linear low-density polyethylene - hexene comonomer (LLDPE-C6) with low-density polyethylene (LDPE) excellent mechanical resistance, along .. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 5.00 kg, Temperature 372 °C |
1.0 g/10 min @Load 11.0 lb, Temperature 702 °F |
ASTM D1238 |
3M Dyneon™ FEP X 6301 UHP Fluorothermoplastic Fluorinated Ethylene Propylene
(discontinued **) Dyneon FEP X 6301 UHP was designed primarily for ultra-high purity applications requiring very low levels of metals and ions. This extrusion grade of EEP is ideally suited for tubing, which can be u.. |
|||
Melt Index of Compound | 1.0 g/10 min @Temperature 190 °C |
1.0 g/10 min @Temperature 374 °F |
ASTM D1238 |
Mitsui ADMER® NF458A PE Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |
|||
Melt Index of Compound | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
Lushan M-10D Adhesive Resin for Multi-layer Sausage Casing film Adhesive resin Lushan series for sausages casing film is anhydride-modified polyethylene product and is available in pellet form. Adhesive resin Lushan series for sausages casing film is designed fo.. |
|||
Melt Index of Compound | 1.0 - 3.0 g/10 min | 1.0 - 3.0 g/10 min | |
Sibur ABS 1106 Extrusion Grade ABS Plastic With high deformation properties and sanitary-hygienic properties for production of sheets with following pneumatic and vacuum forming of internal parts of refrigerators, as well as for compounding .. |
|||
Melt Index of Compound | 1.0 g/10 min | 1.0 g/10 min | |
Sibur MPP 15-06V Frost Resistant Polypropylene For production of parts for automobiles (bumpers), accumulators, articles of technical purpose, including those electrical and exploited under low temperatures |
|||
Melt Index of Compound | 1.0 g/10 min | 1.0 g/10 min | |
Sibur MPP 21015-E10 Frost Resistant Polypropylene For production of parts for automobiles (bumpers), accumulators, articles of technical purpose, including those electrical and exploited under low temperatures |
|||
Melt Index of Compound | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 524E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 524E is an extrusion grade olefinic thermoplastic elastomer. This mineral filled product is suited for profile extrusion or blow molding. TPP 524E is paintable and can be .. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
A. Schulman FORMION™ FI 105E Non-Reinforced, Extrusion Grade Sodium Ionomer DescriptionFormion® FI 1051E is a non-reinforced, transparent, extrusion grade Sodium Ionomer. It has been formulated for high durability, cut and puncture resistance, and low temperature ductilit.. |
|||
Melt Index of Compound | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 524E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 524E is an extrusion grade olefinic thermoplastic elastomer. This mineral filled product is suited for profile extrusion or blow molding. TPP 524E is paintable and can be .. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
Cond. E; ISO 1133 |
A. Schulman FORMION™ FI 388 Ionomer Information provided by A. Schulman. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
A. Schulman FORMION™ FI 105E Non-Reinforced, Extrusion Grade Sodium Ionomer DescriptionFormion® FI 1051E is a non-reinforced, transparent, extrusion grade Sodium Ionomer. It has been formulated for high durability, cut and puncture resistance, and low temperature ductilit.. |
|||
Melt Index of Compound | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 1010E-01 Olefinic Elastomer For Sheet Extrusion DescriptionPolytrope TPP 1010E-01 is an olefinic elastomer designed for sheet extrusion, profile extrusion and blow molding. TPP 1010E-01 is a natural product which can be colored and UV stabilized.. |
|||
Melt Index of Compound | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 524E Extrusion Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 524E is an extrusion grade olefinic thermoplastic elastomer. This mineral filled product is suited for profile extrusion or blow molding. TPP 524E is paintable and can be .. |
|||
Melt Index of Compound | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 1010E-01 Olefinic Elastomer For Sheet Extrusion DescriptionPolytrope TPP 1010E-01 is an olefinic elastomer designed for sheet extrusion, profile extrusion and blow molding. TPP 1010E-01 is a natural product which can be colored and UV stabilized.. |
|||
Melt Index of Compound | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 1010E-01 Olefinic Elastomer For Sheet Extrusion DescriptionPolytrope TPP 1010E-01 is an olefinic elastomer designed for sheet extrusion, profile extrusion and blow molding. TPP 1010E-01 is a natural product which can be colored and UV stabilized.. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
Cond. E; ISO 1133 |
A. Schulman FORMION™ FI 388 Ionomer Information provided by A. Schulman. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow Engage® 8100 Polyolefin Elastomer Description: Engage® 8100 polyolefin elastomer is an ethyleneoctene copolymer that has excellent flow characteristics and performs well in a wide range of general purpose thermoplastic elastomer ap.. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow FLEXOMER™ DFDA-1137 NT 7 Very Low Density Polyethylene (VLDPE) Resin FLEXOMER™ DFDA-1137 NT 7 is an ethylene copolymer intended for use in molding and extrusion applications where high flexibility is desired. It is especially useful for flexible hose and tube appli.. |
|||
Melt Index of Compound | 1.0 - 1.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 - 1.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group LOTRYL® 7 BA 01 Copolymer Ethylene - Butyl Acrylate LOTRYL® 7 BA 01 is a random copolymer of ethylene and butyl acrylate, prepared by the high pressure polymerization process. LOTRYL® 7 BA 01 is used for film coextrusion and lamination where sealab.. |
|||
Melt Index of Compound | 1.0 - 1.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 - 1.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Arkema Group OREVAC® C306 Maleic Anhydride Modified Linear Low Density Polyethylene OREVAC C306 is anhydride modified LLDPE. It is available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylene (PE) resins. It has been designed.. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 5.00 kg, Temperature 372 °C |
1.0 g/10 min @Load 11.0 lb, Temperature 702 °F |
ASTM D1238 |
3M Dyneon™ FEP 6301Z Fluorinated Ethylene Propylene Fluorothermoplastic Granules Dyneon FEP 6301Z is offered for extrusion, injection molding and transfer molding for the wire and cable and chemical process industries. Their distinguishing features include: Excellent electrical .. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYfill PPC T1020 Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
Cond. E; ISO 1133 |
A. Schulman FORMION™ FI 388 Ionomer Information provided by A. Schulman. |
|||
Melt Index of Compound | 1.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
A. Schulman FORMION™ FI 105E Non-Reinforced, Extrusion Grade Sodium Ionomer DescriptionFormion® FI 1051E is a non-reinforced, transparent, extrusion grade Sodium Ionomer. It has been formulated for high durability, cut and puncture resistance, and low temperature ductilit.. |
|||
Melt Index of Compound | 1.0 g/10 min | 1.0 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 1010E-01 Olefinic Elastomer For Sheet Extrusion DescriptionPolytrope TPP 1010E-01 is an olefinic elastomer designed for sheet extrusion, profile extrusion and blow molding. TPP 1010E-01 is a natural product which can be colored and UV stabilized.. |