Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 0.90 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.90 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trilene® TS 5009 LLDPE-C4 and LDPE Blend The Trilene TS 5009 product is a blend with a high ratio of linear low-density polyethylene (LLDPE) with low-density polyethylene (LDPE) with elevated processability, ensuring the production of film.. |
|||
Melt Index of Compound | 0.90 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.90 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trilene® TS 8057 LLDPE-C4 and LDPE Blend The Trilene® TS 8057 product is a blend with a high ratio of linear low-density polyethylene - butene copolymer (LLDPE) with low-density polyethylene (LDPE) providing elevated processability and en.. |
|||
Melt Index of Compound | 0.90 g/10 min @Load 3.80 kg, Temperature 230 °C |
0.90 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
LG Chemical HI835HS PMMA, Impact Resistant Grade Molding granule designed for greater impact strength combined with the outstanding properties of conventional acrylic materialsFeatures: Excellent transparency and eleganceWeather resistance and che.. |
|||
Melt Index of Compound | 0.90 g/10 min @Temperature 190 °C |
0.90 g/10 min @Temperature 374 °F |
ASTM D1238 |
Mitsui ADMER® SF700A Elastomer Type Polyolefin ADMER® Adhesive Resin is a modified polyolefin with functional groups, designed to bond to a variety of polyolefins, ionomers, polyamides, ethylene vinyl alcohol (EVOH), polyesters (PET), polycar.. |
|||
Melt Index of Compound | 0.90 g/10 min | 0.90 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 408 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 408 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Melt Index of Compound | 0.90 g/10 min | 0.90 g/10 min | ASTM D1238 |
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl.. |
|||
Melt Index of Compound | 0.90 g/10 min | 0.90 g/10 min | LE 4421; ASTM D1238 |
Borealis Visico™/Ambicat™ LE4421/LE4476 Ambient Curing, Moisture-Crosslinking Polyethylene Compound for Low Voltage Insulation Visico LE4421 is a natural, ethylene vinyl silane copolymer that, when combined with the catalyst masterbatch Ambicat LE4472, will undergo an accelerated, moisture-induced crosslinking reaction. Th.. |
|||
Melt Index of Compound | 0.90 g/10 min | 0.90 g/10 min | LE 4423; ASTM D1238 |
Borealis Visico™/Ambicat™ LE4423/LE4472 Black, Fast Curing, Silane Crosslinkable LDPE Compound for Weather Resistant Covering/Insulation of Overhead Cables Visico LE4423 is a natural, ethylene vinyl silane copolymer that, when combined with the catalyst masterbatch Ambicat LE4472, will undergo an accelerated, moisture-induced crosslinking reaction. Th.. |
|||
Melt Index of Compound | 0.90 g/10 min | 0.90 g/10 min | ASTM D1238 |
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl.. |
|||
Melt Index of Compound | 0.90 g/10 min | 0.90 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 408 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 408 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Melt Index of Compound | 0.90 g/10 min | 0.90 g/10 min | ASTM D1238 |
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl.. |
|||
Melt Index of Compound | 0.90 g/10 min | 0.90 g/10 min | ASTM D1238 |
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl.. |
|||
Melt Index of Compound | 0.90 g/10 min | 0.90 g/10 min | ASTM D1238 |
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl.. |
|||
Melt Index of Compound | 0.90 g/10 min | 0.90 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 408 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 408 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Melt Index of Compound | 0.90 g/10 min | 0.90 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 408 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 408 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Melt Index of Compound | 0.90 g/10 min | 0.90 g/10 min | ASTM D1238 |
A. Schulman CP842-01 Hexene Copolymer LLDPE Resin DescriptionCP 842-01 is a Hexene copolymer LLDPE resin designed for use in blown film applications. Blow up ratios of2:1 or higher are recommended. ApplicationTypical applications of CP 842-01 incl.. |
|||
Melt Index of Compound | 0.90 g/10 min | 0.90 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 408 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 408 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Melt Index of Compound | 0.90 g/10 min @Load 2.16 kg, Temperature 190 °C |
0.90 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D-1238 |
Chevron Phillips Marlex® C300 Polyethylene; Enhanced Metallocene medium density polyethylene. This metallocene MDPE resin is tailored for blow molded containers that require: High glossGood clarityExcellent ESCR Applications: Typical blow molded ap.. |
|||
Melt Index of Compound | 0.90 g/10 min | 0.90 g/10 min | ASTM D1238 |
A. Schulman POLYTROPE™ TPP 408 Blow Molding Grade Olefinic Thermoplastic Elastomer DescriptionPolytrope TPP 408 is a blow molding grade olefinic thermoplastic elastomer. This elastomer is specifically designed for flexible, automotive under-hood air ducts. This product contains .. |
|||
Melt Index of Compound | 0.90 g/10 min | 0.90 g/10 min | LE 4421; ASTM D1238 |
Borealis Visico™/Ambicat™ LE4421/LE4472 Ambient Curing, Moisture-Crosslinking Polyethylene Compound for Low Voltage Insulation Visico LE4421 is a natural, ethylene vinyl silane copolymer that, when combined with the catalyst masterbatch Ambicat LE4472, will undergo an accelerated, moisture-induced crosslinking reaction. Th.. |
|||
Melt Index of Compound | 0.90 g/10 min | 0.90 g/10 min | LE 4423; ASTM D1238 |
Borealis Visico™/Ambicat™ LE4423/LE4476 Fast Curing, Easy Processing, Environmentally Friendly, Silane Crosslinkable LDPE Compound for Low Voltage Insulation Visico LE4423 is a natural, ethylene vinyl silane copolymer that, when combined with the catalyst masterbatch Ambicat LE4472, will undergo an accelerated, moisture-induced crosslinking reaction. Th.. |