Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 50 g/10 min @Load 5.00 kg, Temperature 260 °C |
50 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Polykemi AB POLYblend C65F PC/ABS-blend Information provided by Polykemi AB |
|||
Melt Index of Compound | 50 g/10 min @Load 5.00 kg, Temperature 260 °C |
50 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Polykemi AB POLYblend C65HF PC/ABS-blend Information provided by Polykemi AB |
|||
Melt Index of Compound | 50 g/10 min @Load 10.0 kg, Temperature 190 °C |
50 g/10 min @Load 22.0 lb, Temperature 374 °F |
MVR, [cm<sup>3</sup>/10 min] |
Huntsman IROGRAN® A 75 P 4655 N TPU-Polyester Introduction: IROGRAN A 75 P 4655 N is a black colored polyether based thermoplastic polyurethane intended for injection molding applications. IROGRAN A 75 P 4655 N is a part of the HUNTSMAN injecti.. |
|||
Melt Index of Compound | 50 g/10 min @Load 21.6 kg, Temperature 190 °C |
50 g/10 min @Load 47.6 lb, Temperature 374 °F |
cm<sup>3</sup>/10 min |
Huntsman IROGRAN® A 78 E 4723 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 78 E 4723 is a thermoplastic polyester- polyurethane for injection moulding and extrusion applications. Additional characteristics of the product are flexibility and high mec.. |
|||
Melt Index of Compound | 50 g/10 min @Load 21.6 kg, Temperature 190 °C |
50 g/10 min @Load 47.6 lb, Temperature 374 °F |
MVR, [cm<sup>3</sup>/10 min] |
Huntsman IROGRAN® A 85 H 4508 TPU-Polyester Introduction: IROGRAN A 85 H 4508 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are excellent mechanical properties and hig.. |
|||
Melt Index of Compound | 50 g/10 min @Load 21.6 kg, Temperature 190 °C |
50 g/10 min @Load 47.6 lb, Temperature 374 °F |
cm<sup>3</sup>/10 min |
Huntsman IROGRAN® A 85 P 4350 TPU-Polyether Introduction: IROGRAN A 85 P 4350 is a flame-retardant, halogen-free, thermoplastic polyether-polyurethane intended for extrusion and injection molding applications. Additional characteristics of th.. |
|||
Melt Index of Compound | 50 g/10 min @Load 21.6 kg, Temperature 190 °C |
50 g/10 min @Load 47.6 lb, Temperature 374 °F |
cm<sup>3</sup>/10 min |
Huntsman IROGRAN® A 85 P 4380 TPU-Polyether Introduction: IROGRAN A 85 P 4380 is a flame-retardant, halogen-free, thermoplastic polyether-polyurethane intended for extrusion and injection molding applications. Additional characteristics of th.. |
|||
Melt Index of Compound | 50 g/10 min @Load 21.6 kg, Temperature 190 °C |
50 g/10 min @Load 47.6 lb, Temperature 374 °F |
cm<sup>3</sup>/10 min |
Huntsman IROGRAN® A 87 H 4615 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 87 H 4615 is a thermoplastic polyester- polyurethane for injection molding applications. Additional characteristics of the product are very short cycle times and high dimensi.. |
|||
Melt Index of Compound | 50 g/10 min @Load 2.16 kg, Temperature 190 °C |
50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICOFLOâ„¢ 510-5028 400 Micron LLDPE Powder Description: ICOFLO 510-5028 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melt Index of Compound | 50 g/10 min @Load 2.16 kg, Temperature 190 °C |
50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICOFLOâ„¢ 510-5073 500 Micron LLDPE Powder Description: ICOFLO 510-5073 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melt Index of Compound | 50 g/10 min @Load 2.16 kg, Temperature 190 °C |
50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICOFLOâ„¢ 510-5074 800 Micron LLDPE Powder Description: ICOFLO 510-5074 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melt Index of Compound | 50 g/10 min @Load 2.16 kg, Temperature 190 °C |
50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICOFLOâ„¢ 510-5075 1200 Micron LLDPE Powder Description: ICOFLO 510-5075 is a premium polyethylene powder specifically designed to be used in the preparation of masterbatch (concentrate). By utilizing a free flowing powder as a carrier in ma.. |
|||
Melt Index of Compound | 50 g/10 min @Load 21.6 kg, Temperature 190 °C |
50 g/10 min @Load 47.6 lb, Temperature 374 °F |
cm<sup>3</sup>/10 min |
Huntsman IROGRAN® A 80 H 4698 Polyester-Based TPU-Injection Molding Grade Introduction: IROGRAN A 80 H 4698 is a transparent thermoplastic polyester-polyurethane for injection molding applications. Additional characteristics of the product are good melt flow and easy demo.. |
|||
Melt Index of Compound | 50 g/10 min @Load 5.00 kg, Temperature 315 °C |
50 g/10 min @Load 11.0 lb, Temperature 599 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics LNP LUBRICOMP OCL13XXP PPS - LINEAR (Europe-Africa-Middle East) LNP* Stat-kon* OCL13XXP is a compound based on PPS - LINEAR resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Melt Index of Compound | 50 g/10 min @Load 10.0 kg, Temperature 300 °C |
50 g/10 min @Load 22.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics LNP STAT-KON DX07323 PC+ABS (Asia Pacific) LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, .. |
|||
Melt Index of Compound | 50 g/10 min @Load 10.0 kg, Temperature 300 °C |
50 g/10 min @Load 22.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics LNP STAT-KON DX07323 PC+ABS (Europe-Africa-Middle East) LNP* STAT-KON* DX07323 is a compound based on polycarbonate resin containing conductive fillers. Added features of this compound includes: ESD safe and excellent low-temperature impact performance, .. |
|||
Melt Index of Compound | 50 g/10 min | 50 g/10 min | Condition E; ASTM D1238 |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
Melt Index of Compound | 50 g/10 min | 50 g/10 min | Condition E; ASTM D1238 |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
Melt Index of Compound | 50 g/10 min | 50 g/10 min | Condition E; ASTM D1238 |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
Melt Index of Compound | 50 g/10 min | 50 g/10 min | Condition E; ASTM D1238 |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
Melt Index of Compound | 50 g/10 min | 50 g/10 min | Condition E; ASTM D1238 |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
Melt Index of Compound | 50 g/10 min | 50 g/10 min | Condition E; ASTM D1238 |
A. Schulman CP814-01 Linear, Low-Density Polyethylene DescriptionCP 814-01 is a linear low-density polyethylene resin with excellent molding characteristics and good low temperature impact. ApplicationCP814-01 meets the specifications contained in FDA .. |
|||
Melt Index of Compound | 50 g/10 min @Load 2.16 kg, Temperature 190 °C |
50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow DNDA-7147 NT 7 Linear Low Density Polyethylene Resin DOW DNDA-7147 NT 7 is produced using UNIPOL™ PE process technology. It is intended for use in injection molding applications such as food containers, housewares and lids. Information provided by D.. |
|||
Melt Index of Compound | 50 g/10 min @Load 2.16 kg, Temperature 190 °C |
50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Dow DOWLEX™ IP-51 High Density Polyethylene Resin (HDPE) DOWLEX™ IP-51 is an Improved Processing high density resin designed to offer excellent process-ability and impact performance. This resin was designed by optimization of the breadth, shape and pea.. |
|||
Melt Index of Compound | 50 g/10 min @Load 2.16 kg, Temperature 230 °C |
50 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Dow R7021-50RNA Polypropylene Random Copolymer Resin DOW™ R7021-50RNA Polypropylene Resin is a random copolymer designed for thin wall injection molding applications desiring high clarity.Main CharacteristicsGood impact propertiesExcellent opticsFast.. |