Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 5.8 - 7.2 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.8 - 7.2 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Petroquimica Triunfo Trithene® CX 7065 LDPE - Extrusion Coating The Trithene® CX 7065 resin is a product developed especially to meet the segment of extrusion coating where the following properties are necessary: processing stability at high production rates, a.. |
|||
Melt Index of Compound | 5.8 g/10 min @Load 3.80 kg, Temperature 230 °C |
5.8 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
LG Chemical IG840 PMMA, General Purpose Grade for Injection Molding General purpose grade with better flowability than IH 830 but slightly below in heat resistanceMechanical strength and surface hardnessFeatures: Excellent transparency and eleganceWeather resistance.. |