Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 28 g/10 min @Load 10.0 kg, Temperature 220 °C |
28 g/10 min @Load 22.0 lb, Temperature 428 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycolac® FR30U ABS (Asia Pacific) Flame retardant ABS. Good indoor UV properties. Excellent moldability with no bloom. V-1/V-0/5VB rated. |
|||
Melt Index of Compound | 28 g/10 min @Load 21.6 kg, Temperature 190 °C |
28 g/10 min @Load 47.6 lb, Temperature 374 °F |
cm<sup>3</sup>/10 min |
Huntsman IROGRAN® A 85 D 4968 Polyester-Based TPU-Injection Extrusion Grade High Hydrolysis resistance and good crystallinity. Suggested for extrusion.Information provided by Huntsman |
|||
Melt Index of Compound | 28 g/10 min @Load 5.00 kg, Temperature 360 °C |
28 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM EXUM0167 PEI Blend Improved ductility, transparent, standard flow Polyetherimide blend (Tg 200C) with internal mold release and enhanced ductility. ECO Conforming. |
|||
Melt Index of Compound | 28 g/10 min @Load 2.16 kg, Temperature 190 °C |
28 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Sterigenics Raprex® R-400C Thermoplastic Powder Applications: Extrusion CoatingsA thermoplastic powder based on polyethylene was developed by Sterigenics Advanced Applications for extrusion coating on metal and other surfaces. RAPREX™ 400 is.. |
|||
Melt Index of Compound | 28 g/10 min @Load 5.00 kg, Temperature 300 °C |
28 g/10 min @Load 11.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ASTM D1238 |
SABIC Innovative Plastics LNP THERMOCOMP DF00A8P PC (Asia Pacific) LNP* Thermocomp* DF00A8P is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good impact perform.. |
|||
Melt Index of Compound | 28 g/10 min @Load 5.00 kg, Temperature 224 °C |
28 g/10 min @Load 11.0 lb, Temperature 435 °F |
ASTM D1238 |
Dow PELLETHANE® 2103-75D Film Grade Thermoplastic Polyurethane Elastomer
(discontinued **) Description: PELLETHANE® 2103-75D UV stabilized, polyether based thermoplastic polyurethane elastomer has excellent hydrolytic stability and excellent resistance to micro-organisms. Applications in.. |