Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 21 g/10 min @Load 2.16 kg, Temperature 260 °C |
21 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CX2142ME PC+ABS Cycoloy* resin grade CX2142ME is an injection moldable PC/ABS blend with Br- and Cl-free flame retardant systems. Key features of good flow, good impact, UL-94 V0 rating at 1.2 mm, and improved chem.. |
|||
Melt Index of Compound | 21 g/10 min @Load 2.16 kg, Temperature 260 °C |
21 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CX7110 PC+ABS Cycoloy* resin grade CX7110 is an injection moldable PC/ABS blend with non-brominated and non-chlorinated flame retardant systems. Excellent impact/flow balance together with a UL-94 V0 rating at 1... |
|||
Melt Index of Compound | 21 g/10 min @Load 5.00 kg, Temperature 260 °C |
21 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CY9640 PC+ABS (Asia Pacific) PC+ ABS, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 121 PC (Europe-Africa-Middle East) LEXAN 121 is a low viscosity multi purpose grade available in transparent, translucent and opaque colours. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 915AU PC (Europe-Africa-Middle East) LEXAN resin grade 915AU is a flame retardant polycarbonate featuring non brominated and non chlorinated FR systems, with good flow, and good UV stability. It is available in transparent colors, inte.. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 920 PC (Europe-Africa-Middle East) LEXAN 920 is a low viscosity flame retardant grade, especially suitable for electrical applications. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® FXD123R PC (Europe-Africa-Middle East) LEXAN FXD123R is a transparent/translucent low viscosity grade for light diffusion special effects. UV-stabilized. Color package may affect performance. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® FXE121R PC (Europe-Africa-Middle East) LEXAN FXE121R is a transparent/translucent low viscosity grade for special effects colors with a fluorescent appearance. Color package may affect performance. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® FXG121R PC (Europe-Africa-Middle East) LEXAN FXG121R is a transparent/translucent low viscosity grade for special effects colors with a diamond sparkle appearance. Color package may affect performance. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® FXM121R PC (Europe-Africa-Middle East) LEXAN FXM121R is a transparent/translucent low viscosity grade for special effects colors with a metallic-luster appearance. Color package may affect performance. |
|||
Melt Index of Compound | 21 g/10 min @Load 5.00 kg, Temperature 220 °C |
21 g/10 min @Load 11.0 lb, Temperature 428 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® LI1813R PC Low-viscosity multi-purpose PC having low levels of ionics species. Internal mold release and UV-stabilized. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® LI1911R PC (Europe-Africa-Middle East) Low-viscosity multi-purpose grade having low levels of ionics species. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® OQ4120R PC (Europe-Africa-Middle East) Optical grade with UV cut-off up to 400 nm, greater optical purity than standard grades. For needs of sunglass and sunvisor markets. MFR of 25. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® PC2200 PC (Asia Pacific) PC2200 resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product designed for use in the custom compounding market. It does not contain UV stabilizer or mold release. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® PC2200R PC (Europe-Africa-Middle East) PC2200R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® VR1820 PC (Europe-Africa-Middle East) VR1820 resin is a high flow (MFR = 22 at 300ºC/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Melt Index of Compound | 21 g/10 min @Load 2.16 kg, Temperature 260 °C |
21 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CX2142ME PC+ABS (Europe-Africa-Middle East) Cycoloy* resin grade CX2142ME is an injection moldable PC/ABS blend with Br- and Cl-free flame retardant systems. Key features of good flow, good impact, UL-94 V0 rating at 1.2 mm, and improved chem.. |
|||
Melt Index of Compound | 21 g/10 min @Load 2.16 kg, Temperature 190 °C |
21 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm3/10 min; ISO 1133 |
DuPont Performance Polymers Delrin® FG900P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG900P is a low viscosity acetal homopolymer, with improved thermal stability. It has been developed for consideration into applications such as parts for the food industry.Information prov.. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics PC2200R PC (Europe-Africa-Middle East) PC2200R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Melt Index of Compound | 21 g/10 min @Load 1.20 kg, Temperature 300 °C |
21 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics PC2203R PC (Asia Pacific) PC2203R resin is a high flow (MFR = 22 at 300?C/1.2kg), heat and UV stabilized, polycarbonate product with mold release designed for use in the general purpose molding market. |
|||
Melt Index of Compound | 21 g/10 min @Load 5.00 kg, Temperature 360 °C |
21 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM HU1110 PEI Enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Melt Index of Compound | 21 g/10 min @Load 5.00 kg, Temperature 360 °C |
21 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM HU1110 PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Melt Index of Compound | 21 g/10 min @Load 2.16 kg, Temperature 250 °C |
21 g/10 min @Load 4.76 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® IQ325HP PBT (Asia Pacific) FDA compliant PBT resin, using chemically recycled post consumer PET Bottles. Fit to food contact applications. |
|||
Melt Index of Compound | 21 g/10 min @Load 2.16 kg, Temperature 265 °C |
21 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics XYLEX X7300 PC+POLYESTER PC+POLYESTER unreinforced alloy. High flow, chemically resistant with excellent optical quality. UV-stabilized. |
|||
Melt Index of Compound | 21 g/10 min @Load 2.16 kg, Temperature 265 °C |
21 g/10 min @Load 4.76 lb, Temperature 509 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics XYLEX X7300 PC+POLYESTER (Europe-Africa-Middle East) PC+POLYESTER unreinforced alloy. High flow, chemically resistant with excellent optical quality. UV-stabilized. |
|||
Melt Index of Compound | 21 - 25 g/10 min | 21 - 25 g/10 min | |
Sibur 21230 Polypropylene Compounding for stabilization 16K, 16V, 16N, 16M, 16H superior quality. For production of technical and domestic products of complicated profile, of non-woven materials. |
|||
Melt Index of Compound | 21 g/10 min @Load 5.00 kg, Temperature 300 °C |
21 g/10 min @Load 11.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL NH5120C PPE+PS (Asia Pacific) Noryl* NH5120C resin is a modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, good chemical resistance, and low specifc gravity for light weight parts. The .. |
|||
Melt Index of Compound | 21 g/10 min @Load 2.16 kg, Temperature 250 °C |
21 g/10 min @Load 4.76 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® V3004 PBT (Asia Pacific) Unfilled PBT modified with elastomer. Targeted for flexible hinge, automotive connectors, film applications. |
|||
Melt Index of Compound | 21 g/10 min | 21 g/10 min | ASTM D1238 |
Cheng Yu Plastic 3245 TPE Rubber |
|||
Melt Index of Compound | 21 g/10 min @Load 10.0 kg, Temperature 300 °C |
21 g/10 min @Load 22.0 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics LNP KONDUIT PX11313 PA 6 (Europe-Africa-Middle East) Thermally conductive mineral and glass fiber filled PA6, FR, compliant with ECO protocols, non-brominated, non-chlorinated |