Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 19.76 g/10 min @Load 10.0 kg, Temperature 220 °C |
19.76 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
LG Chemical HI-121 ABS, High Impact Feature: Injection Molding, Well Balanced Mechanical PropertiesApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information Provided by LG Chem |