Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 13 g/10 min @Load 2.16 kg, Temperature 230 °C |
13 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Polykemi AB POLYelast TPE RCZ350D UV4 Thermoplastic Elastomer, UV-Resistant Information provided by Polykemi AB |
|||
Melt Index of Compound | 13 g/10 min @Load 5.00 kg, Temperature 260 °C |
13 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CP8320 PC+ABS Cycoloy Medium Heat Plating Grade for Automotive |
|||
Melt Index of Compound | 13 g/10 min @Load 5.00 kg, Temperature 260 °C |
13 g/10 min @Load 11.0 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Cycoloy® CY6414 PC (Europe-Africa-Middle East) Flame retardant modified PC blend using non-brominated and non-chlorinated flame retardant systems, offering high heat for application in appliances, lighting and electrical market. |
|||
Melt Index of Compound | 13 g/10 min @Load 2.16 kg, Temperature 260 °C |
13 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics GELOY HRA222 ASA (Asia Pacific) GELOY HRA222 is a multi-purpose, chlorine and bromine free flame retardant PC+ASA alloy for injection molding processes. Use for exterior/interior electrical applications requiring UV resistance. |
|||
Melt Index of Compound | 13 g/10 min @Load 2.16 kg, Temperature 260 °C |
13 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics GELOY HRA222F ASA+PC (Asia Pacific) Geloy HRA222F is a multi-purpose, chlorine and bromine free flame retardant PC+ASA alloy for injection molding processes. F1 rating according UL746C. Use for exterior/interior electrical application.. |
|||
Melt Index of Compound | 13 g/10 min @Load 2.16 kg, Temperature 260 °C |
13 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics GELOY HRA222F ASA+PC (Europe-Africa-Middle East) Geloy HRA222F is a multi-purpose, chlorine and bromine free flame retardant ASA-PC alloy for injection moulding processes. This grade has a F1 rating according UL746C. Typical properties as measured.. |
|||
Melt Index of Compound | 13 g/10 min @Load 1.20 kg, Temperature 300 °C |
13 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer (Asia Pacific) This product will be phased out per January 2015 -- Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance. |
|||
Melt Index of Compound | 13 g/10 min @Load 1.20 kg, Temperature 300 °C |
13 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 925 PC (Europe-Africa-Middle East) Lexan* 925A Polycarbonate (PC) resin is a non-filled, injection moldable grade of non-chlorinated, non-brominated flame retardant systems that has an UL-94 V0 rating. Lexan 925A is available in tran.. |
|||
Melt Index of Compound | 13 g/10 min @Load 1.20 kg, Temperature 300 °C |
13 g/10 min @Load 2.65 lb, Temperature 572 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Lexan® 925AU PC (Europe-Africa-Middle East) Lexan* 925AU Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is UV stabilized, providing addit.. |
|||
Melt Index of Compound | 13 g/10 min @Load 2.16 kg, Temperature 190 °C |
13 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm3/10 min; ISO 1133 |
DuPont Performance Polymers Delrin® 511DP BK402 Acetal Homopolymer
(Unverified Data**) Delrin® 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided.. |
|||
Melt Index of Compound | 13 g/10 min @Load 2.16 kg, Temperature 190 °C |
13 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ICO Polymers ICORENEâ„¢ 440-1312 PP Rotational Molding Resin Description: ICORENE 440-1312 is a polypropylene copolymer developed for rotational molding applications. The resin is fully UV protected. Key Characteristics: very high rigidity, good creep resist.. |
|||
Melt Index of Compound | 13 g/10 min @Load 5.00 kg, Temperature 280 °C |
13 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL WCV072 PPE+PP (Europe-Africa-Middle East) Flexible, halogen free mPPE extrusion grade material for applications such as automotive wire insulation. Low specific gravity with good flame retardant and very good scrape abrasion resistance. De.. |
|||
Melt Index of Compound | 13 g/10 min @Load 5.00 kg, Temperature 360 °C |
13 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 1000R PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. UL94 V0, V2 and 5VA listing. |
|||
Melt Index of Compound | 13 g/10 min @Load 5.00 kg, Temperature 220 °C |
13 g/10 min @Load 11.0 lb, Temperature 428 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 1000RV PEI Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. |
|||
Melt Index of Compound | 13 g/10 min @Load 5.00 kg, Temperature 340 °C |
13 g/10 min @Load 11.0 lb, Temperature 644 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 1010FC PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant. Effective June, 2007 this grade will no longer be support.. |
|||
Melt Index of Compound | 13 g/10 min @Load 5.00 kg, Temperature 340 °C |
13 g/10 min @Load 11.0 lb, Temperature 644 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 1010M PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. |
|||
Melt Index of Compound | 13 g/10 min @Load 5.00 kg, Temperature 360 °C |
13 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 4001 PEI (Europe-Africa-Middle East) PTFE filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. |
|||
Melt Index of Compound | 13 g/10 min @Load 5.00 kg, Temperature 360 °C |
13 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM PW1000 PEI (Europe-Africa-Middle East) Unfilled Standard flow Polyetherimide (Tg 217°C). Specific grade-colors aredesigned and certified for use in Potable Water applications. KTW, WRAS, ACS, NSF-61 and W270 certified. US FDA and Euro.. |
|||
Melt Index of Compound | 13 g/10 min @Load 2.16 kg, Temperature 260 °C |
13 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® 830F PBT+PET PBT+PET, 30% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
Melt Index of Compound | 13 g/10 min @Load 2.16 kg, Temperature 260 °C |
13 g/10 min @Load 4.76 lb, Temperature 500 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Valox® 830F PBT+PET (Asia Pacific) PBT+PET, 30% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
Melt Index of Compound | 13 g/10 min @Load 5.00 kg, Temperature 250 °C |
13 g/10 min @Load 11.0 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Xenoy® CL101 PBT+PC Xenoy CL101 is an unfilled, impact modified PC/PBT blend with excellent solvent resistance and low-temperature ductility. It has a proven track record in off-line painted exterior automotive applica.. |
|||
Melt Index of Compound | 13 g/10 min @Load 2.16 kg, Temperature 250 °C |
13 g/10 min @Load 4.76 lb, Temperature 482 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics Xenoy® X5100 PC+PBT (Europe-Africa-Middle East) XENOY X5100 is a semi-crystalline, impact modified PC-PBT blend with excellent flow. (PC+PBT-I). |
|||
Melt Index of Compound | 13 g/10 min @Load 5.00 kg, Temperature 280 °C |
13 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance. |
|||
Melt Index of Compound | 13 g/10 min @Load 5.00 kg, Temperature 280 °C |
13 g/10 min @Load 11.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA (Asia Pacific) NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance. |
|||
Melt Index of Compound | 13 g/10 min @Load 5.00 kg, Temperature 360 °C |
13 g/10 min @Load 11.0 lb, Temperature 680 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM 1000P PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C) in 350 micron powder. Resin is RoHS compliant. |
|||
Melt Index of Compound | 13 g/10 min @Load 5.00 kg, Temperature 340 °C |
13 g/10 min @Load 11.0 lb, Temperature 644 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics ULTEM AUT200M PEI (Europe-Africa-Middle East) Transparent high flow Polyetherimide (Tg 217C) with internal mold release.. Very low outgassing and plateout, for automotive lighting applications where highly metallized, reflective surfaces are re.. |
|||
Melt Index of Compound | 13 g/10 min @Load 10.0 kg, Temperature 280 °C |
13 g/10 min @Load 22.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. This grade has been certified for potable water applications up to 85C in Europe and North America, color .. |
|||
Melt Index of Compound | 13 - 19 g/10 min @Temperature 230 °C |
13 - 19 g/10 min @Temperature 446 °F |
ASTM D1238 |
A. Schulman POLYFLAM™ CFP 4623 20% Calcium Filled Polypropylene DescriptionPolyfort® 4623 is a 20% calcium filled polypropylene.Information provided by A. Schulman. |
|||
Melt Index of Compound | 13 g/10 min @Load 10.0 kg, Temperature 280 °C |
13 g/10 min @Load 22.0 lb, Temperature 536 °F |
MVR [cm^3/10 min]; ISO 1133 |
SABIC Innovative Plastics NORYL GFN1520V PPE+HIPS (Asia Pacific) NORYL GFN1520V is a 20% glass fibre reinforced material with improved hydrolytic stability. This grade has been certified for potable water applications up to 85C in Europe and North America, color .. |
|||
Melt Index of Compound | 13 g/10 min | 13 g/10 min | cm3/10 min; ISO 1133 |
DuPont Performance Polymers Delrin® 527UVE NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 527UVE NC010 (formerly DE20556) is a medium viscosity acetal homopolymer with UV stabilizers having extremely low VOC emissions, developed for automotive interior applications.Information p.. |