Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm3/10 min; ISO 1133 |
DuPont Performance Polymers Delrin® 150 NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has excellent thermal stability, low die deposit, and enhanced crystallization for low porosity.Information pr.. |
|||
Melt Index of Compound | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Dow 359.00 Developmental Performance Polypropylene Polymer Dow Announced Sale of Global Polypropylene Business to Braskem in July 2011. |
|||
Melt Index of Compound | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Dow 6D20 Polypropylene Random Copolymer Resin OverviewConsistent processabilityGood regrind stabilityGood gloss and clarityLow odor and taste transferComplies with: U.S. FDA 21 CFR 177.1520 (c)3.1a, Europe EU-Directive 2002/72/ECDOW 6D20 Polypr.. |
|||
Melt Index of Compound | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Dow 6D83K Polypropylene Random Copolymer Resin OverviewConsistent processabilityLow odor and taste transferHigh glossGood regrind stabilityContains clarifying additiveComplies with: U.S. FDA 21 CFR 177.1520 (c)3.2a, Canadian HPFB No ObjectionDOW.. |
|||
Melt Index of Compound | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Dow C133-02 Polypropylene Impact Copolymer Resin OverviewDow C133-02 Polypropylene Resin is intended for use in extrusion, thermoforming, and extrusion blow molding applications where impact at refrigeration temperatures is desired. It is especia.. |
|||
Melt Index of Compound | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Dow R131-02A Polypropylene Random Copolymer Resin DOW R131-02A Polypropylene Resin is a random copolymer intended for use in extrusion blow molding applications. The product can be used in both single layer and multilayer designs including barrier.. |
|||
Melt Index of Compound | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm3/10 min; ISO 1133 |
DuPont Performance Polymers Delrin® 111P NC010 Acetal Homopolymer Delrin® 111P is a high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, fewer voids). It has higher tensile strength and mod.. |
|||
Melt Index of Compound | 1.9 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Dow R132-02A Polypropylene Random Copolymer Resin DOW R132-02A Polypropylene Resin is a random copolymer intended for use in extrusion blow molding applications. The product can be used in both single layer and multilayer designs including barrier.. |
|||
Melt Index of Compound | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm3/10 min; ISO 1133 |
DuPont Performance Polymers Delrin® FG150 NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG150 NC010 is a high viscosity acetal homopolymer for extrusion processes. It has low die deposit and low porosity. It has been developed for consideration in applications and parts for th.. |
|||
Melt Index of Compound | 1.9 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.9 g/10 min @Load 4.76 lb, Temperature 374 °F |
cm3/10 min; ISO 1133 |
DuPont Performance Polymers Delrin® FG100P NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG100P is a high viscosity acetal homopolymer, with improved thermal stability for use in easy to fill molds. It has been developed for consideration into applications such as parts for the.. |