Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Index of Compound | 1.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
carrier resin value; ASTM D-1238 |
Chevron Phillips MarFlex® ER3341 Polyethylene; Masterbatch
(discontinued **) Metallocene polyethylene antiblock masterbatch. This antiblock concentrate with its mLLDPE carrier is tailored for use with mPACT™ resins in blown film applications that require: Reduced COFMinim.. |
|||
Melt Index of Compound | 1.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
carrier resin value; ASTM D-1238 |
Chevron Phillips MarFlex® ER3343 Polyethylene; Masterbatch
(discontinued **) Metallocene polyethylene slip masterbatch. This erucamide slip concentrate with its mLLDPE carrier is tailored for use with mPact™ resins in blown film applications that require: Reduced COFExcel.. |
|||
Melt Index of Compound | 1.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
carrier resin value; ASTM D-1238 |
Chevron Phillips MarFlex® ER3344 Polyethylene; Masterbatch
(discontinued **) Metallocene polyethylene antiblock masterbatch. This erucamide slip and antiblock concentrate with its mLLDPE carrier is tailored for use with mPACT™ resins in blown film applications that require.. |
|||
Melt Index of Compound | 1.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D-1238 |
Chevron Phillips MarFlex® 7114 Polyethylene; LLDPE Hexene linear low density polyethylene. This LLDPE is tailored for applications that require: Good stiffness at thin gaugesGood drawdownExcellent processabilityCan use straight or in blends with L.. |
|||
Melt Index of Compound | 1.4 g/10 min @Load 2.16 kg, Temperature 190 °C |
1.4 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D-1238 |
Chevron Phillips Marlex® C101 Polyethylene; Enhanced Metallocene linear low density polyethylene. This linear low density, hexene copolymer is tailored for blow molded containers that require: High glossGood clarityExcellent ESCR Applications: Typi.. |