Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage = 0.018 in/in Product List

Physical Properties

Tips: 30 items are displayed at most.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0090 - 0.018 cm/cm
<br>@Thickness 1.60 mm
0.0090 - 0.018 in/in
<br>@Thickness 0.0630 in
horizontal; ASTM D955
Gromax CCP PBT 1100-220S
Product Description: PBT unreinforced and impact-modified injection molding grade. Characteristics:Low warp age, high toughness and excellent dimensional stabilityExcellent glossy surface and less-g..
Linear Mold Shrinkage 0.0090 - 0.018 cm/cm
<br>@Thickness 1.60 mm
0.0090 - 0.018 in/in
<br>@Thickness 0.0630 in
horizontal; ASTM D955
Gromax PBT 2000-104D
Product Description: PBT unreinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Excellent mechanic an..
Linear Mold Shrinkage 0.0090 - 0.018 cm/cm
<br>@Thickness 1.60 mm
0.0090 - 0.018 in/in
<br>@Thickness 0.0630 in
horizontal; ASTM D955
Gromax PBT 2000-201D
Product Description: PBT unreinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature. Excellent mechanic an..
Linear Mold Shrinkage 0.010 - 0.018 cm/cm
<br>@Thickness 1.60 mm
0.010 - 0.018 in/in
<br>@Thickness 0.0630 in
vertical; ASTM D955
Gromax PBT 2100-104B
Product Description: PBT unreinforced flame-retarded injection molding grade. Characteristics:Excellent electrical property Excellent mechanic and chemical property Excellent weatherability Excellen..
Linear Mold Shrinkage 0.012 - 0.018 cm/cm
<br>@Thickness 1.60 mm
0.012 - 0.018 in/in
<br>@Thickness 0.0630 in
vertical; ASTM D955
Gromax PBT 3020-104 15% Glass Fiber Filled
Product Description: A glass fiber 20% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent ..
Linear Mold Shrinkage 0.014 - 0.018 cm/cm
<br>@Thickness 3.00 mm
0.014 - 0.018 in/in
<br>@Thickness 0.118 in
Absolute Drying
Toyobo GLAMIDE® NB-5620S Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.014 - 0.018 cm/cm
<br>@Thickness 3.00 mm
0.014 - 0.018 in/in
<br>@Thickness 0.118 in
DAM
Toyobo NB-5620S Nylon/Olefin Alloy, 15% Mineral Reinforced (Conditioned)
Features: 15% Mineral Reinforced, Light WeightInformation provided by Toyobo.
Linear Mold Shrinkage 0.014 - 0.018 cm/cm
<br>@Thickness 3.00 mm
0.014 - 0.018 in/in
<br>@Thickness 0.118 in
Toyobo NB-5620S Nylon/Olefin Alloy, 15% Mineral Reinforced (DAM)
Features: 15% Mineral Reinforced, Light WeightInformation provided by Toyobo.
Linear Mold Shrinkage 0.014 - 0.018 cm/cm
<br>@Thickness 3.00 mm
0.014 - 0.018 in/in
<br>@Thickness 0.118 in
Absolute Drying
Toyobo GLAMIDE® NB-1700 Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Linear Mold Shrinkage 0.016 - 0.018 cm/cm
<br>@Thickness 3.17 mm
0.016 - 0.018 in/in
<br>@Thickness 0.125 in
Direction of Flow; ASTM D955
Diamond Polymers Softflex® 6001 Thermoplastic Elastomer Alloy
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Linear Mold Shrinkage 0.016 - 0.018 cm/cm
<br>@Thickness 3.17 mm
0.016 - 0.018 in/in
<br>@Thickness 0.125 in
Transverse to Flow; ASTM D955