Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.017 - 0.020 cm/cm @Thickness 3.20 mm |
0.017 - 0.020 in/in @Thickness 0.126 in |
Flow, 24h; ASTM D955 |
DuPont Performance Polymers Delrin® 500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 500AL is a medium viscosity acetal homopolymer, with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel, itself or other plas.. |
|||
Linear Mold Shrinkage | 0.017 - 0.020 cm/cm @Thickness 3.20 mm |
0.017 - 0.020 in/in @Thickness 0.126 in |
Transverse, 24h; ASTM D955 |
DuPont Performance Polymers Delrin® 500AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 500AL is a medium viscosity acetal homopolymer, with an advanced system of lubrication for applications requiring low wear and/or coefficient of friction against steel, itself or other plas.. |
|||
Linear Mold Shrinkage | 0.017 - 0.020 cm/cm @Thickness 3.17 mm |
0.017 - 0.020 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® PP-60/V2 Polypropylene Homopolymer, Flame Retardant, UL94 V2 Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.018 - 0.020 cm/cm @Thickness 3.17 mm |
0.018 - 0.020 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® PP-60/VO Polypropylene Homopolymer, Flame Retardant, UL94 V0 Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm @Thickness 1.60 mm |
0.014 - 0.020 in/in @Thickness 0.0630 in |
vertical; ASTM D955 |
Gromax PBT 4115-104D 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm @Thickness 1.60 mm |
0.014 - 0.020 in/in @Thickness 0.0630 in |
vertical; ASTM D955 |
Gromax PBT 3015-201 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.015 - 0.020 cm/cm @Thickness 3.00 mm |
0.015 - 0.020 in/in @Thickness 0.118 in |
Absolute Drying |
Toyobo GLAMIDE® TY-102ND Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.017 - 0.020 cm/cm @Thickness 3.20 mm |
0.017 - 0.020 in/in @Thickness 0.126 in |
Transverse, 24h; ASTM D955 |
DuPont Performance Polymers Delrin® 111P NC010 Acetal Homopolymer Delrin® 111P is a high viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, fewer voids). It has higher tensile strength and mod.. |
|||
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm @Thickness 1.60 mm |
0.014 - 0.020 in/in @Thickness 0.0630 in |
vertical; ASTM D955 |
Gromax CCP PBT 4815-NCB 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm @Thickness 1.60 mm |
0.014 - 0.020 in/in @Thickness 0.0630 in |
vertical; ASTM D955 |
Gromax PBT 3015-104 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm @Thickness 1.60 mm |
0.014 - 0.020 in/in @Thickness 0.0630 in |
vertical; ASTM D955 |
Gromax PBT 4115-201D 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |