Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.014 cm/cm @Thickness 6.40 mm |
0.014 in/in @Thickness 0.252 in |
Flow; DAM |
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66
(Unverified Data**) Minlon® 11C40 BKB086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage | 0.014 cm/cm @Thickness 6.40 mm |
0.014 in/in @Thickness 0.252 in |
Transverse; DAM |
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66
(Unverified Data**) Minlon® 11C40 BKB086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage | 0.014 cm/cm @Thickness 6.35 mm |
0.014 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® PP-60/TC/10 Polypropylene Homopolymer, 10% Talc Filled Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.014 - 0.016 cm/cm @Thickness 6.35 mm |
0.014 - 0.016 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® PP-61/CC/20 Polypropylene Copolymer, 20% Calcium Carbonate Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.014 - 0.016 cm/cm @Thickness 6.35 mm |
0.014 - 0.016 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® PP-62/CC/20/UV Polypropylene Copolymer, 20% Calcium Carbonate, UV Stabilized Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm @Thickness 1.60 mm |
0.014 - 0.020 in/in @Thickness 0.0630 in |
vertical; ASTM D955 |
Gromax PBT 4115-104D 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm @Thickness 1.60 mm |
0.014 - 0.020 in/in @Thickness 0.0630 in |
vertical; ASTM D955 |
Gromax PBT 3015-201 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.014 - 0.018 cm/cm @Thickness 3.00 mm |
0.014 - 0.018 in/in @Thickness 0.118 in |
Absolute Drying |
Toyobo GLAMIDE® NB-5620S Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.014 - 0.018 cm/cm @Thickness 3.00 mm |
0.014 - 0.018 in/in @Thickness 0.118 in |
DAM |
Toyobo NB-5620S Nylon/Olefin Alloy, 15% Mineral Reinforced (Conditioned) Features: 15% Mineral Reinforced, Light WeightInformation provided by Toyobo. |
|||
Linear Mold Shrinkage | 0.014 - 0.018 cm/cm @Thickness 3.00 mm |
0.014 - 0.018 in/in @Thickness 0.118 in |
|
Toyobo NB-5620S Nylon/Olefin Alloy, 15% Mineral Reinforced (DAM) Features: 15% Mineral Reinforced, Light WeightInformation provided by Toyobo. |
|||
Linear Mold Shrinkage | 0.014 - 0.018 cm/cm @Thickness 3.00 mm |
0.014 - 0.018 in/in @Thickness 0.118 in |
Absolute Drying |
Toyobo GLAMIDE® NB-1700 Nylon/Olefin GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.014 cm/cm @Thickness 3.20 mm |
0.014 in/in @Thickness 0.126 in |
Flow |
DuPont Performance Polymers Crastin® T835FRUV NC010 PBT Crastin® T835FRUV NC010 is a 5% glass fiber reinforced, toughened, flame retardant polybutylene terephthalate resin for injection molding. (precommercial code = Crastin® CE2402)Information provide.. |
|||
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm @Thickness 1.60 mm |
0.014 - 0.020 in/in @Thickness 0.0630 in |
vertical; ASTM D955 |
Gromax CCP PBT 4815-NCB 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm @Thickness 1.60 mm |
0.014 - 0.020 in/in @Thickness 0.0630 in |
vertical; ASTM D955 |
Gromax PBT 3015-104 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |
|||
Linear Mold Shrinkage | 0.014 - 0.020 cm/cm @Thickness 1.60 mm |
0.014 - 0.020 in/in @Thickness 0.0630 in |
vertical; ASTM D955 |
Gromax PBT 4115-201D 15% Glass Fiber Filled Product Description: A glass fiber 15% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |