Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0017 cm/cm @Thickness 1.57 mm |
0.0017 in/in @Thickness 0.0618 in |
Flow |
DuPont Performance Polymers Rynite® 940 BK505 PET
(Unverified Data**) Rynite® 940 BK505 is a 40% mica/glass reinforced modified polyethylene terephthalate with greater strength, stiffness, and low warpage.Information provided by DuPont Performance Polymers |