Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.015 cm/cm @Thickness 6.40 mm |
0.015 in/in @Thickness 0.252 in |
Flow; DAM |
DuPont Performance Polymers Minlon® 12TA BKB124 Nylon 66
(Unverified Data**) Minlon® 12TA BKB124 is a 32% mineral reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage | 0.015 cm/cm @Thickness 6.40 mm |
0.015 in/in @Thickness 0.252 in |
Transverse; DAM |
DuPont Performance Polymers Minlon® 12TA BKB124 Nylon 66
(Unverified Data**) Minlon® 12TA BKB124 is a 32% mineral reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage | 0.015 - 0.022 cm/cm @Thickness 3.00 mm |
0.015 - 0.022 in/in @Thickness 0.118 in |
Absolute Drying |
Toyobo GLAMIDE® T-656E Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.015 - 0.022 cm/cm @Thickness 3.00 mm |
0.015 - 0.022 in/in @Thickness 0.118 in |
Absolute Drying |
Toyobo GLAMIDE® T-662 Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.015 - 0.020 cm/cm @Thickness 3.00 mm |
0.015 - 0.020 in/in @Thickness 0.118 in |
Absolute Drying |
Toyobo GLAMIDE® TY-102ND Nylon/Elastomer GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.015 - 0.022 cm/cm @Thickness 3.00 mm |
0.015 - 0.022 in/in @Thickness 0.118 in |
DAM |
Toyobo T-661 Nylon 66, Standard Grade (Conditioned) Features: Non-reinforced, Standard GradeInformation provided by Toyobo. |
|||
Linear Mold Shrinkage | 0.015 - 0.022 cm/cm @Thickness 3.00 mm |
0.015 - 0.022 in/in @Thickness 0.118 in |
|
Toyobo T-661 Nylon 66, Standard Grade (DAM) Features: Non-reinforced, Standard GradeInformation provided by Toyobo. |
|||
Linear Mold Shrinkage | 0.015 cm/cm @Temperature 240 °C |
0.015 in/in @Temperature 464 °F |
ASTM D3392 |
DuPont™ Nomex® Type 993, 60 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ.. |
|||
Linear Mold Shrinkage | 0.015 cm/cm @Thickness 3.20 mm |
0.015 in/in @Thickness 0.126 in |
Transverse; DAM |
DuPont Performance Polymers Zytel® FE4200 BK136 Nylon 66
(Unverified Data**) Zytel® FE4200 BK136 is a low die deposit polyamide 66 extrusion resin.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage | 0.015 cm/cm @Thickness 1.27 mm |
0.015 in/in @Thickness 0.0500 in |
Transverse; ASTM D955 |
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET
(Unverified Data**) Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac.. |
|||
Linear Mold Shrinkage | 0.015 cm/cm @Diameter 4.00 mm |
0.015 in/in @Diameter 0.157 in |
Normal |
DuPont Performance Polymers Delrin® 300ATB BK000 Acetal Homopolymer
(Unverified Data**) Delrin® 300ATB BK000 is a filled, medium viscosity, toughened acetal homopolymer for injection molding. It is well suited for antistatic applications.Information provided by DuPont Performance Poly.. |