Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0040 cm/cm @Thickness 3.20 mm |
0.0040 in/in @Thickness 0.126 in |
Flow; DAM |
DuPont Performance Polymers Minlon® 10B40HS1 BK061 Nylon 66
(Unverified Data**) Minlon® 10B40HS1 BK061 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage | 0.0040 cm/cm @Thickness 3.17 mm |
0.0040 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® J-60/10/FR Polypropylene Homopolymer, 10% Glass Reinforced, Flame Retardant Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0040 cm/cm @Thickness 6.35 mm |
0.0040 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® J-60/20/E8 Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0040 cm/cm @Thickness 6.35 mm |
0.0040 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® J-60/20/H Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0040 cm/cm @Thickness 6.35 mm |
0.0040 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® J-60/30/E3 Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0040 cm/cm @Thickness 6.35 mm |
0.0040 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® J-60/30/E8/M Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0040 cm/cm @Thickness 6.35 mm |
0.0040 in/in @Thickness 0.250 in |
ASTM D955 |
Fiberfil® J-60/20/E/HF Polypropylene Homopolymer, 20% Glass Reinforced, Chemically coupled, improved flow Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0040 - 0.0070 cm/cm @Thickness 3.00 mm |
0.0040 - 0.0070 in/in @Thickness 0.118 in |
Absolute Drying |
Toyobo GLAMIDE® T-402 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0070 cm/cm @Thickness 1.00 mm |
0.0040 - 0.0070 in/in @Thickness 0.0394 in |
Absolute Drying |
Toyobo GLAMIDE® T-803 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0080 cm/cm @Thickness 1.00 mm |
0.0040 - 0.0080 in/in @Thickness 0.0394 in |
Absolute Drying |
Toyobo GLAMIDE® T-808-02 Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
48 hr at 80°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0040 - 0.0060 cm/cm @Thickness 3.20 mm |
0.0040 - 0.0060 in/in @Thickness 0.126 in |
72 hr; ASTM D955 |
A. Schulman POLYPUR™ FPU 1550 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0040 cm/cm @Thickness 6.40 mm |
0.0040 in/in @Thickness 0.252 in |
Flow; DAM |
DuPont Performance Polymers Zytel® 77G33HS1L NC010 Nylon 612 Zytel® 77G33HS1L NC010 is a 33% glass fiber reinforced, heat stabilized polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage | 0.0040 cm/cm @Thickness 3.20 mm |
0.0040 in/in @Thickness 0.126 in |
Flow; DAM |
DuPont Performance Polymers Minlon® FE6190 BK086 Nylon 66 Minlon® FE6190 BK086 is a 36% mineral/glass reinforced, heat stabilized, black polyamide resin for injection molding.Information provided by DuPont Performance Polymers |