Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0020 cm/cm @Thickness 3.17 mm |
0.0020 in/in @Thickness 0.125 in |
ASTM D955 |
Fiberfil® J-60/40 Polypropylene Homopolymer, 40% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
48 hr at 121°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
48 hr at 121°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0030 cm/cm @Thickness 1.00 mm |
0.0020 - 0.0030 in/in @Thickness 0.0394 in |
Absolute Drying |
Toyobo GLAMIDE® TY-145TZ Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
48 hr at 121°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1377 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0040 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0040 in/in @Thickness 0.126 in |
48 hr at 121°C; ASTM D955 |
A. Schulman POLYPUR™ FPU 1376 Thermoplastic Polyurethane Compound Information provided by A. Schulman. |
|||
Linear Mold Shrinkage | 0.0020 cm/cm @Thickness 3.20 mm |
0.0020 in/in @Thickness 0.126 in |
Flow |
DuPont Performance Polymers Rynite® 408 NC010 PET Rynite® 408 NC010 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness, and temperature resistance.Inf.. |
|||
Linear Mold Shrinkage | 0.0020 - 0.0050 cm/cm @Thickness 1.60 mm |
0.0020 - 0.0050 in/in @Thickness 0.0630 in |
horizontal; ASTM D955 |
Gromax CCP PBT 5630-200C 30% Glass Fiber Filled Product Description: A glass fiber 30% reinforced injection molding grade. Characteristics:Excellent electrical property Excellent temperature resistance, high heat distortion temperature Excellent .. |