Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 3.00 g/cc @Temperature 200 °C |
0.108 lb/in³ @Temperature 392 °F |
|
Sharadaa Ceramics Sharada RFC-95 Gel Bonded Castables Mullite Bonded Free Flowing Cement Free Versatile Castable SystemProduct Characteristics: High Mullitisation, Free from Low Temperature eutectics, Non wetting to molten metals Ferrous/Non Ferrous, E.. |