Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Transverse = 0.0400 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00210 - 0.0400 cm/cm
0.00210 - 0.0400 in/in
Average value: 0.0208 cm/cm Grade Count:102
Overview of materials for Acetal Copolymer, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of..
Linear Mold Shrinkage, Transverse 0.00800 - 0.0400 cm/cm
0.00800 - 0.0400 in/in
Average value: 0.0140 cm/cm Grade Count:25
Overview of materials for Acetal Copolymer, 30% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% ar..
Linear Mold Shrinkage, Transverse 0.0165 - 0.0400 cm/cm
0.0165 - 0.0400 in/in
Average value: 0.0225 cm/cm Grade Count:3
Overview of materials for Acetal Copolymer, Aramid Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va..
Linear Mold Shrinkage, Transverse 0.00200 - 0.0400 cm/cm
0.00200 - 0.0400 in/in
Average value: 0.0111 cm/cm Grade Count:94
Overview of materials for Nylon 610
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Linear Mold Shrinkage, Transverse 0.000500 - 0.0400 cm/cm
0.000500 - 0.0400 in/in
Average value: 0.00932 cm/cm Grade Count:180
Overview of materials for Nylon 12
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en..
Linear Mold Shrinkage, Transverse 0.0100 - 0.0400 cm/cm
0.0100 - 0.0400 in/in
Average value: 0.0188 cm/cm Grade Count:10
Overview of materials for Nylon 66, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, PTFE Filled". Each property range of values reported is minimum and maximum values of appropri..
Linear Mold Shrinkage, Transverse 0.0100 - 0.0400 cm/cm
0.0100 - 0.0400 in/in
Average value: 0.0197 cm/cm Grade Count:12
Overview of materials for Acetal Copolymer, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu..
Linear Mold Shrinkage, Transverse 0.00200 - 0.0400 cm/cm
0.00200 - 0.0400 in/in
Average value: 0.0143 cm/cm Grade Count:17
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..
Copyright © lookpolymers.com All Rights Reserved