Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00160 - 0.0300 cm/cm | 0.00160 - 0.0300 in/in | Average value: 0.0152 cm/cm Grade Count:14 |
Overview of materials for Polybutylene Terephthalate (PBT), Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Impact Grade". Each property range of values reported is minimum and m.. |
|||
Linear Mold Shrinkage, Transverse | 0.00170 - 0.0300 cm/cm | 0.00170 - 0.0300 in/in | Average value: 0.0116 cm/cm Grade Count:27 |
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an.. |
|||
Linear Mold Shrinkage, Transverse | 0.000 - 0.0300 cm/cm | 0.000 - 0.0300 in/in | Average value: 0.0137 cm/cm Grade Count:4 |
Overview of materials for Polycarbonate-Urethane This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate-Urethane". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Linear Mold Shrinkage, Transverse | 0.00900 - 0.0300 cm/cm | 0.00900 - 0.0300 in/in | Average value: 0.0164 cm/cm Grade Count:11 |
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar.. |
|||
Linear Mold Shrinkage, Transverse | 0.0100 - 0.0300 cm/cm | 0.0100 - 0.0300 in/in | Average value: 0.0198 cm/cm Grade Count:4 |
Overview of materials for Acetal Copolymer, Silicone Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Silicone Filled". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage, Transverse | 0.00600 - 0.0300 cm/cm | 0.00600 - 0.0300 in/in | Average value: 0.0143 cm/cm Grade Count:12 |
Overview of materials for Acetal Copolymer, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Carbon Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Linear Mold Shrinkage, Transverse | 0.0200 - 0.0300 cm/cm | 0.0200 - 0.0300 in/in | Average value: 0.0249 cm/cm Grade Count:3 |
Overview of materials for Acetal Copolymer, Steel Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Steel Filled". Each property range of values reported is minimum and maximum values of.. |
|||
Linear Mold Shrinkage, Transverse | 0.0100 - 0.0300 cm/cm | 0.0100 - 0.0300 in/in | Average value: 0.0189 cm/cm Grade Count:61 |
Overview of materials for Acetal Homopolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced". Each property range of values reported is minimum and maximum values .. |
|||
Linear Mold Shrinkage, Transverse | 0.00800 - 0.0300 cm/cm | 0.00800 - 0.0300 in/in | Average value: 0.0226 cm/cm Grade Count:6 |
Overview of materials for Polyvinylidinefluoride (PVDF), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyvinylidinefluoride (PVDF), Molded/Extruded". Each property range of values reported is minimum and m.. |
|||
Linear Mold Shrinkage, Transverse | 0.00960 - 0.0300 cm/cm | 0.00960 - 0.0300 in/in | Average value: 0.0162 cm/cm Grade Count:7 |
Overview of materials for High Density Polyethylene (HDPE), Injection Molded This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Injection Molded". Each property range of values reported is minimum a.. |
|||
Linear Mold Shrinkage, Transverse | 0.0100 - 0.0300 cm/cm | 0.0100 - 0.0300 in/in | Average value: 0.0141 cm/cm Grade Count:3 |
Overview of materials for Acetal Copolymer + Glass/PTFE This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer + Glass/PTFE". Each property range of values reported is minimum and maximum values of .. |
|||
Linear Mold Shrinkage, Transverse | 0.00250 - 0.0300 cm/cm | 0.00250 - 0.0300 in/in | Average value: 0.00686 cm/cm Grade Count:60 |
Overview of materials for Polyethersulfone (PES) This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Linear Mold Shrinkage, Transverse | 0.00110 - 0.0300 cm/cm | 0.00110 - 0.0300 in/in | Average value: 0.0132 cm/cm Grade Count:94 |
Overview of materials for Nylon 6, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced". Each property range of values reported is minimum and maximum values of appropri.. |