Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.017 - 0.023 cm/cm
0.017 - 0.023 in/in
ISO DIS 294-4
Wellman Wellamid® NY1615-BK Unfilled Nylon 66
Description: Unfilled Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Transverse 0.019 - 0.023 cm/cm
0.019 - 0.023 in/in
ISO DIS 294-4
Wellman Wellamid® XT1482-BK High Impact Nylon 66
Description: High Impact Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Transverse 0.019 - 0.023 cm/cm
0.019 - 0.023 in/in
ISO DIS 294-4
Wellman Wellamid® XT1606-N Impact Modified Nylon 66
Description: Impact Modified Nylon 66Information provided by Wellman.
Linear Mold Shrinkage, Transverse 0.0080 - 0.023 cm/cm
0.0080 - 0.023 in/in
Flame Bar; ASTM D955
DSM Biomedical PurSil® 20 Thermoplastic Silicone Polyether Polyurethane (TSPU)
A novel copolymer that is strong yet flexible with proven biocompatibility and biostability Combining the benefits of both silicone elastomers and polyether urethanes, PurSil® TSPU has exceptional..
Linear Mold Shrinkage, Transverse 0.019 - 0.023 cm/cm
0.019 - 0.023 in/in
DIS 294-4
Wellman Wellamid® 22L-NBK1/WE-1434 Nylon 66, Engineering Grade
All information provided by Wellman Engineered Resins.