Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0065 cm/cm @Thickness 3.20 mm |
0.0045 - 0.0065 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 3412HF PC 20% glass reinforced, high flow PC. UL rated V-1 at 0.059"", |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0065 cm/cm | 0.0050 - 0.0065 in/in | |
LATI Kelon® B FR H2 CEG/500-V0CT3 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. Low thermal expansion co.. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0065 cm/cm | 0.0040 - 0.0065 in/in | |
LATI Larpeek 10 G/50 PEEK, 50% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0065 cm/cm | 0.0045 - 0.0065 in/in | |
LATI Larton G/40 PPS, 40% Glass Fiber Reinforced Polyphenylene Sulfide (PPS) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0065 cm/cm | 0.0045 - 0.0065 in/in | |
LATI Lastilac SP G/17 ABS, Glass Fiber Reinforced Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. Glass fibers. High dimensional stability.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInforma.. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0065 cm/cm | 0.0040 - 0.0065 in/in | |
LATI Kelon® B FR H CETG/250-V0 PA 6, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers / Mineral filler. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacifi.. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0065 cm/cm | 0.0040 - 0.0065 in/in | |
LATI Kelon® B H CET/30 PA 6, 30% Mineral Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. Very high dimensional stability. Good elongationAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; North Amer.. |
|||
Linear Mold Shrinkage, Transverse | 0.0040 - 0.0065 cm/cm | 0.0040 - 0.0065 in/in | |
LATI Laramid G/60 PPA, 60% Glass Fiber Reinforced Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; .. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0065 cm/cm | 0.0045 - 0.0065 in/in | |
LATI Laril 13 G/30 PPOm, 30% Glass Fiber Reinforced Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. Low thermal expansion coefficient. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; .. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0065 cm/cm | 0.0045 - 0.0065 in/in | |
LATI Laril 13 G/30-V1 PPOm, 30% Glass Fiber Reinforced, Flame Retardant Modified Polyphenylene Oxide (PPOm) based compound. Glass fibers. UL94 V-1 classified, with brominated flame retardants, PBB/PBDE and antimony trioxide free. High dimensional stability. Good thermal.. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0065 cm/cm | 0.0045 - 0.0065 in/in | |
LATI Lastilac AR-V0E ABS, Flame Retardant Acrylonitrile-Butadiene-Styrene copolymer (ABS) based compound. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free. Very high dimensional stability. Very good surface appearance.Av.. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0065 cm/cm | 0.0050 - 0.0065 in/in | |
LATI Laticonther 75 CPG/650 PBT, Glass Fiber Reinforced High thermal conductivity product based on Polybutylene Terephthalate (PBT). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInfor.. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0065 cm/cm | 0.0045 - 0.0065 in/in | |
LATI Latilub 87/28-12T G/20 PC, 20% Glass Fiber Reinforced, PTFE Filled Self-lubricating product based on Polycarbonate (PC). PTFE. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria .. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0065 cm/cm @Thickness 3.20 mm |
0.0045 - 0.0065 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Noryl_NC2525 PPE+HIPS (Europe-Africa-Middle East) LNP* Stat-kon* Noryl_NC2525 compound is a 25% CFR PPE+PS. Highly conductive. High heat. May be added to similar material/regrind to add some conductivity to the blend. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0065 cm/cm @Thickness 3.20 mm |
0.0045 - 0.0065 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP STAT-KON Noryl_NC2525 PPE+PS LNP* Stat-kon* Noryl_NC2525 compound is a 25% CFR PPE+PS. Highly conductive. High heat. May be added to similar material/regrind to add some conductivity to the blend. |
|||
Linear Mold Shrinkage, Transverse | 0.0053 - 0.0065 cm/cm @Time 86400 sec |
0.0053 - 0.0065 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-LOY N30009 PC+ABS LNP* STAT-LOY* N30009 is a compound based on PC+ABS Blend resin. Added features of this material include: Antistat, Flame Retardant. |
|||
Linear Mold Shrinkage, Transverse | 0.0060 - 0.0065 cm/cm @Time 86400 sec |
0.0060 - 0.0065 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP DX11354 PC (Asia Pacific) This is a PC compound with good plating, surface and mechanical performance, a good candidate for Laser Direct Structuring applications. |
|||
Linear Mold Shrinkage, Transverse | 0.0053 - 0.0065 cm/cm @Time 86400 sec |
0.0053 - 0.0065 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-LOY N30009 PC+ABS (Asia Pacific) LNP* Stat-loy* N30009 is a compound based on PC+ABS Blend resin containing Flame Retardant, Anti-Static. Added features of this material include: Antistat, Flame Retardant. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0065 cm/cm @Thickness 3.00 mm |
0.0045 - 0.0065 in/in @Thickness 0.118 in |
150x105x3mm; b.o. ISO 2577 |
Covestro Bayblend® FR3005 HG PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0065 cm/cm @Thickness 3.00 mm |
0.0045 - 0.0065 in/in @Thickness 0.118 in |
150x105x3mm; b.o. ISO 2577 |
Covestro Bayblend® FR3009 PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Linear Mold Shrinkage, Transverse | 0.0045 - 0.0065 cm/cm @Thickness 3.20 mm |
0.0045 - 0.0065 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 3412HF PC (Asia Pacific) 20% glass reinforced, high flow PC. UL rated V-1 at 0.059"", |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0065 cm/cm | 0.0050 - 0.0065 in/in | |
LATI Laticonther 57 CPG/550 PPA, Glass Fiber Reinforced High thermal conductivity product based on Semi-aromatic polyamide (PPA). Special filler. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformat.. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0065 cm/cm | 0.0050 - 0.0065 in/in | |
LATI Laticonther 62 CEG/500-V0HF1 PA 6, Glass/Mineral Reinforced, Flame Retardant High thermal conductivity product based on Polyamide 6 (PA6). Glass fibers / Mineral filler. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Availability: Africa & Mid.. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0065 cm/cm | 0.0025 - 0.0065 in/in | |
LATI Latigea B01 I6 Bio-Polymer Bio-Polymer (PLA, PHB, ...). Unfilled. Good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici S.p... |