Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0045 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0045 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® JK500 PC+ABS (Asia Pacific) 10% GR, ECO conforming FR, PC+ABS for thinwall molding applications. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | |
LATI Larpeek 10 K/40 PEEK, 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | |
LATI Larpeek 10 K/40 HM PEEK, 40% Carbon Fiber Reinforced Polyetheretherketone (PEEK) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af.. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0045 cm/cm | 0.0030 - 0.0045 in/in | |
LATI Latamid 6 H2 G/65 PA 6, 65% Glass Fiber Reinforced, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla.. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | |
LATI Laticonther 62 GR/70 PA 6, 70% Graphite Reinforced High thermal conductivity product based on Polyamide 6 (PA6). Graphite.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Te.. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0045 cm/cm | 0.0030 - 0.0045 in/in | |
LATI Laticonther 92 GR/65 PUR, 65% Graphite Reinforced High thermal conductivity product based on Polyurethane (PUR). Graphite. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria .. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | |
LATI Latigloss 57 G/60 F2 PPA, 60% Glass Fiber Reinforced Product with high mechanical properties and exceptional surface finish based on Semi-aromatic polyamide (PPA). Glass fibers. Potentially suitable for food/medical contact application. Availability: .. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | |
LATI Latiohm 85-06 PD01 G/15 PES, 15% Glass Fiber Reinforced Semiconductive/dissipative product based on Polyether Sulfone (PES). Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0045 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0045 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1520A PC LNP* Lubricomp* Lexan_LF1520A compound is a 20% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0045 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0045 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1520A PC (Asia Pacific) 20% glass reinforced/15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Linear Mold Shrinkage, Transverse | 0.0020 - 0.0045 cm/cm @Thickness 3.20 mm |
0.0020 - 0.0045 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1520A PC (Europe-Africa-Middle East) LNP* Lubricomp* Lexan_FL1520 compound is a 20% glass reinforced, 15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0045 cm/cm @Thickness 3.20 mm |
0.0025 - 0.0045 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NF1520 PPE+HIPS (Europe-Africa-Middle East) LNP* Lubricomp* Noryl_NF1520 compound is a 20% glass reinforced, 15% PTFE. Wear resistant; 211F HDT @ 264 psi. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0045 cm/cm @Thickness 3.20 mm |
0.0025 - 0.0045 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NF1520 PPE+PS LNP* Lubricomp* Noryl_NF1520 compound is a 20% glass reinforced, 15% PTFE. Wear resistant; 211F HDT @ 264 psi. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0045 cm/cm @Time 86400 sec |
0.0030 - 0.0045 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON EX03319C PEI (Asia Pacific) LNP* Stat-Kon* EX03319C is a polyetherimide compound reinforced with carbon fiber for good stiffness, dimension stability and has extremely high level of cleanliness for the most demanding applicati.. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0045 cm/cm @Time 86400 sec |
0.0030 - 0.0045 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON ZX08301 PPE (Asia Pacific) Stat-Kon* ZX08301 compound is a high heat compounds with ESD safe and low warpage performance suitable for use in Semiconductor Packaging Applications. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0045 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0045 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS LNP* Thermocomp* Lexan_JK500 compound is a 10% GR, ECO conforming FR, PC+ABS for thinwall molding applications. |
|||
Linear Mold Shrinkage, Transverse | 0.0030 - 0.0045 cm/cm @Thickness 3.20 mm |
0.0030 - 0.0045 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_JK500 PC+ABS (Asia Pacific) 10% GR, ECO conforming FR, PC+ABS for thinwall molding applications. |
|||
Linear Mold Shrinkage, Transverse | 0.0038 - 0.0045 cm/cm @Time 86400 sec |
0.0038 - 0.0045 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON EX08318C PEI (Asia Pacific) LNP* Stat-Kon* EX08318C is a polyetherimide compound reinforced with carbon fiber for good stiffness, dimension stability and has extremely high level of cleanliness for the most demanding applicati.. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0045 cm/cm @Thickness 3.20 mm |
0.0025 - 0.0045 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics NORYL EM7304F PPE+PS 15% glass reinforced, high flow with enhanced polyurethane foam adhesion for instrument panel retainers. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | |
LATI Lastil G/30 SAN, 30% Glass Fiber Reinforced Styrene-Acrylonitrile copolymer (SAN) based compound. Glass fibers. High dimensional stability. High stiffness.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaI.. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | |
LATI Latilub 80-15T K/30 PPS, 30% Carbon Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyphenylene Sulfide (PPS). PTFE. Carbon fiber. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati .. |
|||
Linear Mold Shrinkage, Transverse | 0.0025 - 0.0045 cm/cm | 0.0025 - 0.0045 in/in | |
Solvay Specialty Polymers Ixef® 2060 Polyarylamide (PARA)
(discontinued **) Ixef 2060 is a 55% reinforced, general purpose polyarylamide compound. This compound exhibits improved vibration resistance, low warpage, and excellent surface finish. This grade has excellent prope.. |