Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.030 cm/cm @Time 86400 sec |
0.030 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP LUBRICOMP ML004LS PP LNP* LUBRICOMP* ML004LS is a compound based on Polypropylene resin containing 20% PTFE. Added features of this matLNP* Lubricomp* ML004LS is a compound based on Polypropylene resin containing PTFE... |
|||
Linear Mold Shrinkage, Transverse | 0.030 - 0.050 cm/cm @Time 86400 sec |
0.030 - 0.050 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP STAT-KON RX08408 PA 66 LNP* STAT-KON* RX08404 is a compound based on Nylon 66 containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Linear Mold Shrinkage, Transverse | 0.030 - 0.050 cm/cm @Time 86400 sec |
0.030 - 0.050 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Stat-kon RX08408_NA1D004 PA 66 LNP* Stat-Kon* RX08404_NA1D004 is a compound based on Nylon 66 containing Carbon Powder. Characteristics of this grade include: Electrically Conductive, High Impact.This data was supplied by SABI.. |
|||
Linear Mold Shrinkage, Transverse | 0.030 cm/cm | 0.030 in/in | |
E-Polymers TEKASTER® F100 low-mid viscosity PBT Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe.. |
|||
Linear Mold Shrinkage, Transverse | 0.030 cm/cm | 0.030 in/in | |
E-Polymers TEKASTER® F101F Fast cycle time PBT Injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical performance. Specially G/F reinforced PET has excellent heat resistance, a good.. |
|||
Linear Mold Shrinkage, Transverse | 0.030 cm/cm | 0.030 in/in | |
E-Polymers TEKASTER® F101FR Un-Reinforced Flame Retardant PBT Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe.. |
|||
Linear Mold Shrinkage, Transverse | 0.030 cm/cm | 0.030 in/in | ISO 294-4 |
Azoty Tarnow™ Tarnamid® T-27 MTR Polyamide 6 - Transparent Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Transparent up to maximum 2.5 mm.Tarnamid® has the following main properties.. |
|||
Linear Mold Shrinkage, Transverse | 0.030 cm/cm | 0.030 in/in | |
E-Polymers TEKASTER® F101M Unreinforced impact modified PBT Polyester Resin: TEKASTER is thermoplastic polyester resins (PBT, PET) mostly injection molding. PBT has excellent mechanical properties and well balanced engineering plastics with an electrical pe.. |