Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0148 cm/cm | 0.0148 in/in | STN 64 0808 |
Plastcom SLOVAMID 6 GF 40 Polyamide 6, 40% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 40% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Linear Mold Shrinkage, Transverse | 0.0148 cm/cm | 0.0148 in/in | ISO 2577 |
BASF Ultraform® N2644 Z9 POM + PUR Description: Elastomer modified injection molding grade for applications requiring low modulus. Good acoustic damping.Information provided by BASF |