Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.014 cm/cm | 0.014 in/in | |
Plastcom SLOVALEN PH 49 GF 10 GB 20 PP, 20% glass beads, 10% glass fibre, coupling agent FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 10 % glass fiber and 20% glass beads, contains themodifier of mechanical properties. Increased strength in comparis.. |
|||
Linear Mold Shrinkage, Transverse | 0.014 - 0.016 cm/cm @Thickness 3.18 mm |
0.014 - 0.016 in/in @Thickness 0.125 in |
5" x 0.5" x 0.125"; ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-820 GF30 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-820 GF30 is a medium flow, 30% glass fiber reinforced grade of polyetheretherketone (PEEK). This resin offers higher strength and stiffness properties relative to unreinforced KetaSpire.. |
|||
Linear Mold Shrinkage, Transverse | 0.014 cm/cm @Thickness 3.18 mm |
0.014 in/in @Thickness 0.125 in |
5" x 0.5" x 0.125" bar; ASTM D955 |
Solvay Specialty Polymers KetaSpire® KT-850 Polyetheretherketone (PEEK)
(Unverified Data**) KetaSpire KT-850 is the intermediate-flow grade of unreinforced polyetheretherketone (PEEK) supplied in a natural-color pellet form. KetaSpire PEEK is produced to the highest industry standards and .. |
|||
Linear Mold Shrinkage, Transverse | 0.014 cm/cm | 0.014 in/in | Euronil |
Nilit Nilamid B3 H ZA Unfilled, Low Temperature Impact Resistant PA6 Description: Nilamid B3 H ZA is a NYLON 6 with a low level of impact modification, allowing parts to be snap fitted in a dry-as-molded condition. It also has improved impact strength and elongation,.. |
|||
Linear Mold Shrinkage, Transverse | 0.014 cm/cm @Thickness 2.00 mm |
0.014 in/in @Thickness 0.0787 in |
DAM; ISO 294-4 |
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66
(Unverified Data**) Zytel® FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been developed for consideration into applications such as parts for the food industry.Informat.. |
|||
Linear Mold Shrinkage, Transverse | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | |
LATI Latiblend 5262 PP Homopolymer/PA6 Blend based on Polypropylene homopolymer (PPh) / Polyamide 6 (PA6). Unfilled. High impact resistance. Very good elongation.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |
|||
Linear Mold Shrinkage, Transverse | 0.014 - 0.016 cm/cm | 0.014 - 0.016 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® PP4410 PP, Fire Retardant Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Transverse | 0.014 cm/cm | 0.014 in/in | ASTM D955 |
Teknor Apex Telcar® TL-1269A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Linear Mold Shrinkage, Transverse | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | DIS 294-4 |
Wellman Wellamid® GSF1849-N1 Nylon 66, 40% Glass Sphere/Fiber Reinforced Developmental productAll information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.014 - 0.018 cm/cm | 0.014 - 0.018 in/in | DIS 294-4 |
Wellman Wellamid® MRT1487 N Nylon 66, 32% Mineral Reinforced, Impact Modified All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.014 cm/cm | 0.014 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® 2S 20 nat PA610 Product Description: Grilamid 2S 20 natural is an unmodified medium viscosity polyamide 610 (PA610), designed for injection molding as well as extrusion. It is characterized by the following product.. |
|||
Linear Mold Shrinkage, Transverse | 0.014 cm/cm | 0.014 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® 70K20HSL NC010 Nylon 66
(Unverified Data**) Kevlar® Fiber Reinforced Heat Stabilized Polyamide 66 Zytel 70K20HSL NC010 is a heat stabilized PA66 resin modified with Kevlar aramid fiber for excellent wear resistance.Information provided by Du.. |
|||
Linear Mold Shrinkage, Transverse | 0.014 cm/cm | 0.014 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact ApplicationsZytel FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been develop.. |
|||
Linear Mold Shrinkage, Transverse | 0.014 cm/cm | 0.014 in/in | |
Eurotec® Tecomid® NA40 NL E PA 6.6 lubricated, nucleated Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Linear Mold Shrinkage, Transverse | 0.014 cm/cm | 0.014 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® 101L NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101L NC010 is a lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.014 cm/cm | 0.014 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® 151 NC010 Nylon 612
(Unverified Data**) Unreinforced Polyamide 612Information provided by DuPont Performance Polymers |
|||
Linear Mold Shrinkage, Transverse | 0.014 cm/cm | 0.014 in/in | Eurotec |
Eurotec® Tecomid® NA40 NL E PA6.6, unfilled, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Transverse | 0.014 cm/cm @Thickness 4.00 mm, Time 86400 sec |
0.014 in/in @Thickness 0.157 in, Time 24.0 hour |
|
Arkema Group Pebax® 5533 SP 01 Polyether Block Amide (PEBA) Polyether block amide PEBAX® 5533 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide.. |
|||
Linear Mold Shrinkage, Transverse | 0.014 cm/cm | 0.014 in/in | ISO 294-4 |
Azoty Tarnow™ Tarnamid® T-27 GB30 Polyamide 6 - Glass Beads Reinforced 30% Glass beads reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Linear Mold Shrinkage, Transverse | 0.014 cm/cm | 0.014 in/in | ISO 294-4 |
Azoty Tarnow™ Tarnamid® T-29 Polyamide 6 - Natural Medium-high viscosity extrusion grade for mono or multilayer blown film, including biaxial oriented films, also for production of monofilament; can be used for injection molding and compounding.Tarn.. |
|||
Linear Mold Shrinkage, Transverse | 0.014 cm/cm | 0.014 in/in | ISO 294-4 |
Barlog Plastics KEBATER BF110 PBT, 10% glass fiber reinforced PBT-GF10Information provided by BARLOG plastics GmbH. |
|||
Linear Mold Shrinkage, Transverse | 0.014 cm/cm @Thickness 2.00 mm |
0.014 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla.. |
|||
Linear Mold Shrinkage, Transverse | 0.014 cm/cm | 0.014 in/in | ISO 2577 |
BASF Ultramid® KR 4350 BK 00464 PA6/6T (Dry) Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con.. |
|||
Linear Mold Shrinkage, Transverse | 0.014 cm/cm | 0.014 in/in | ISO 294-4 |
Akro-Plastic Akromid® A3 GF 15 (2418) PA 6.6 Dry, 15% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Linear Mold Shrinkage, Transverse | 0.014 cm/cm @Thickness 2.00 mm |
0.014 in/in @Thickness 0.0787 in |
ISO 294-4 |
Ascend Performance Materials Vydyne® 50BW Nylon 66, Conditioned (2.5% Moisture) Vydyne® 50BW is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a high-viscosity resin. This resin offers a well-balanced comb.. |
|||
Linear Mold Shrinkage, Transverse | 0.014 cm/cm @Thickness 2.00 mm |
0.014 in/in @Thickness 0.0787 in |
|
Aardvark Polymers Aardalloy® 3326 POM Alloy Rotational Molding Resin Aardalloy 3326 is an acetal alloy formulated for enhanced impact resistance and elongation.Aardalloy 3326 maintains the high degree of chemical resistance and low fuel permeation rates of unfilled a.. |
|||
Linear Mold Shrinkage, Transverse | 0.014 cm/cm @Thickness 3.20 mm |
0.014 in/in @Thickness 0.126 in |
|
Unitika EX-1222 PA6, Conditioned High-impact nylonInformation provided by Unitika Ltd. |