Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | |
Plastcom SLOVAMID 66 GF 20 HI PA66, 20% glass beads FeaturesChemically reinforced with 20% glass beeds, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. I.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.013 cm/cm | 0.012 - 0.013 in/in | ASTM D955 |
PolyOne Stat-Tech™ CTX-20SS 107/000 Keytec Blue Polyamide 6/12 Copolymer (Nylon 6/12) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | |
Plastcom SLOVALEN PH 69 GF 30 LS PP, 30% glass fibre, mod. of mech. prop., UV stability FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fibre, contains the modifier of mechanical properties. UV stable. Increased strength in comparison with u.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.014 cm/cm @Thickness 3.18 mm |
0.012 - 0.014 in/in @Thickness 0.125 in |
5" x 0.5" x 0.125" bars; ASTM D955 |
Solvay Specialty Polymers AvaSpire® AV-755 SL45 Polyaryletherketone (PAEK)
(Unverified Data**) AV-755 SL45 is a wear resistant grade of AvaSpire polyaryletherketone (PAEK) designed to provide low wear rates and high pressure-velocity (PV) tolerance in lubricated wear environments. Like the ot.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | |
LyondellBasell Lupolen® 5031 L HDPE, Injection Molding Grade Easy flow, injection molding grade for closures, aerosol pumps, spray nozzles for spray cans, small automotive parts such as the caps on lead/acid batteries, knobs, barrels for writing instruments a.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | ASTM-D1204 |
Kinlead PG14 Bag Grade BOPP Plain Film (thickness: 25 µm) PG14 is a low static, bag grade BOPP plain film. It is transparent, low static, and non heat sealable. It has excellent flatness. One side has corona treatment. It is widely used in gift wrapping an.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | 60x60x2; 250°C / WZ 70°C; 600 bar; ISO 294-4 |
Lanxess Pocan® DP C 1502 000000 PBT + PC PBT + PC, non-reinforced, injection molding, improved impact strength, low tendency to warp, UV-stabilizedInformation provided by LANXESS. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | ASTM D955 |
Multibase Multi-Flex® TPE A 5521 BLK TPE A 5521 is based on Shell's Kraton technology licensed to Multibase. The product is extensively used in automotive and non-automotive applications. Multi-Flex TPE contains Kraton™ G.Data p.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.015 cm/cm | 0.012 - 0.015 in/in | |
LATI Latilub 57-10T Y/15 PPA, Aramid Reinforced Self-lubricating product based on Semi-aromatic polyamide (PPA). PTFE. Aramid fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by La.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.014 cm/cm @Thickness 3.18 mm |
0.012 - 0.014 in/in @Thickness 0.125 in |
ASTM D955 |
Solvay Specialty Polymers AvaSpire® AV-750 GF40 Polyaryletherketone (PAEK), 40% Glass Fiber AvaSpire® AV-750 GF40 is a 40% glass reinforced polyaryletherketone (PAEK) designed to fill the marketplace need for a lower-priced PEEK (polyetheretherketone). This resin provides the typical ch.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.014 cm/cm @Thickness 3.20 mm |
0.012 - 0.014 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Valox® 3706 PBT+PC Impact modified PBT+PC resin. Outdoor enclosure. Not available in all colors. |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.015 cm/cm | 0.012 - 0.015 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® F602G30 Nylon 66, 30% Glass Filled, Fire Retardant, Halogen Free Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.016 cm/cm @Thickness 3.20 mm |
0.012 - 0.016 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Noryl GTX GTX979 PPE+PA (Europe-Africa-Middle East) NORYL GTX979 is a conductive, high heat material. It is especially designed for in- and on-line painted bodypanels and fenders in particular, with conductivity for electro-static painting in an uniq.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 - 0.016 cm/cm | 0.012 - 0.016 in/in | DIS 294-4 |
Wellman Wellamid® NY-4000 Nylon 6, Engineering Grade All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | MCI Method 2 |
Goodfellow TPX® RT31XB Injection Molding Grade Polymethylpentene This grade is highly recommended for injection molding; also for film and fiber extrusion.TPX® is semi-crystalline, transparent, very light and - for a polyolefin - expensive. It has good release c.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® L 25 W 40 X PA12-I Product Description: Grilamid L 25 W 40 X is a flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 40 X is impact modified and heat and UV stabilized. The m.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | ISO 294-4 2577 |
DuPont Performance Polymers Crastin® SK645FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK645FR is a flame retardant 30% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.7.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | Eurotec |
Eurotec® Tecodur® PB70 GR10 NL100 PBT, 10% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | |
Eurotec® Tecomid® NB40 NL E PA 6 lubricated, nucleated Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | Eurotec |
Eurotec® Tecomid® NB40 NL RM PA6, unfilled, MoS2, natural Information provided by Eurotec® |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® L 25 W 10 H X PA12 Product Description: Grilamid L 25 W 10 HX is a semi flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 10 HX is impact modified and heat and UV stabilized.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | ISO 294-4 |
Barlog Plastics KEBAFLEX S 35 A.01 TPE-S, Shore A35, translucent TPE-SInformation provided by BARLOG plastics GmbH. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | ISO 294-4 |
Akro-Plastic Akromid® A3 GF 50 (2423) PA 6.6 Conditioned, 50% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | ISO 294-4 |
Barlog Plastics KEBAFLEX P D55.1 Polyester-Elastomer, Shore D55 TPC-ETInformation provided by BARLOG plastics GmbH. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | Sheet |
BASF Ultradur® B 4040 G2 10% Glass Filled PBT + PET Description: Is a PBT + PET, injection-molding grade containing 10% of glass fibers, for industrial parts, rigid, tough and dimensionally stable, for example for program switches, thermostat parts, .. |
|||
Linear Mold Shrinkage, Transverse | 0.012 cm/cm | 0.012 in/in | DAM; ISO 294-4 2577 |
DuPont Performance Polymers Zytel® RS 3261THSL BK041A Nylon 610
(Unverified Data**) Toughened Renewably Sourced Polyamide 610 Developed for Injection Molding Zytel RS 3261THSL BK041A is a renewably sourced polyamide 610 resin containing a minimum of 47% renewably sourced ingredient.. |