Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.0084 cm/cm
0.0084 in/in
Plastcom SLOVAMID 6 T 30 TS PA6, 30% mineral filling
FeaturesDecreased shrinkage against the BT types, increased heat application. Increased modulus in tension - strength of the material. PA matrix reduction. PA for injection moulding with the content..
Linear Mold Shrinkage, Transverse 0.0084 cm/cm
0.0084 in/in
STN 64 0808
Plastcom SLOVAMID 6 T 30 Polyamide 6, 30% Micronized Talc
FeaturesDecreased shrinkage against the BT types, increased heat application up to 170°C. Increased tensile modulus - strength of the material. PA matrix reduction. Application for tools, fillin..