Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0076 cm/cm | 0.0076 in/in | |
Plastcom SLOVAMID 6 NG GF 45 SGF PA6, improved strength, light stability FeaturesPA 6 for injection moulding, chemically strengthened with 45 % of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-goo.. |
|||
Linear Mold Shrinkage, Transverse | 0.0076 cm/cm | 0.0076 in/in | |
Solvay TECHNYLSTARâ„¢ S 218 MT PA6, 40% mineral filled, DRY Description: TechnylStar Polyamide, 40% mineral filled, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific and North AmericaProduct Appli.. |
|||
Linear Mold Shrinkage, Transverse | 0.0076 cm/cm | 0.0076 in/in | ISO Data |
BASF Ultradur S 4090 G4 LS High Speed BK15077 20% Glass Filled PBT |
|||
Linear Mold Shrinkage, Transverse | 0.0076 cm/cm @Time 86400 sec |
0.0076 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP VERTON RX06097 PA 66 (Europe-Africa-Middle East) LNP* VERTON* RX06097 is a compound based on PA 66 resin containing Long Glass Fiber. Added features include; Easy Molding, UV-Stabilized. |