Linear Mold Shrinkage, Transverse 0.00750 - 0.00900 cm/cm
0.00750 - 0.00900 in/in
Average value: 0.00806 cm/cm Grade Count:8
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. ..
Linear Mold Shrinkage, Transverse 0.00750 - 0.0100 cm/cm
0.00750 - 0.0100 in/in
Average value: 0.00860 cm/cm Grade Count:4
Overview of materials for Nylon 6, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ..
Linear Mold Shrinkage, Transverse 0.00750 - 0.0140 cm/cm
0.00750 - 0.0140 in/in
Average value: 0.0105 cm/cm Grade Count:9
Overview of materials for Nylon 66, Glass Fiber/PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Fiber/PTFE Filled". Each property range of values reported is minimum and maximum values..
Linear Mold Shrinkage, Transverse 0.00750 - 0.0128 cm/cm
0.00750 - 0.0128 in/in
Average value: 0.0113 cm/cm Grade Count:3
Overview of materials for Polypropylene, Long Glass Fiber 50%