Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00160 - 0.0240 cm/cm | 0.00160 - 0.0240 in/in | Average value: 0.0145 cm/cm Grade Count:60 |
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim.. |
|||
Linear Mold Shrinkage, Transverse | 0.00130 - 0.0240 cm/cm | 0.00130 - 0.0240 in/in | Average value: 0.0117 cm/cm Grade Count:88 |
Overview of materials for Nylon 66, Heat Stabilized This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Heat Stabilized". Each property range of values reported is minimum and maximum values of appr.. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.0240 cm/cm | 0.00500 - 0.0240 in/in | Average value: 0.0171 cm/cm Grade Count:8 |
Overview of materials for Nylon 66, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Aramid Fiber Filled". Each property range of values reported is minimum and maximum values of .. |