Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00100 - 0.0190 cm/cm | 0.00100 - 0.0190 in/in | Average value: 0.00861 cm/cm Grade Count:23 |
Overview of materials for Styrenic Elastomer (TES) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro.. |
|||
Linear Mold Shrinkage, Transverse | 0.00600 - 0.0190 cm/cm | 0.00600 - 0.0190 in/in | Average value: 0.0130 cm/cm Grade Count:5 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Linear Mold Shrinkage, Transverse | 0.00400 - 0.0190 cm/cm | 0.00400 - 0.0190 in/in | Average value: 0.0104 cm/cm Grade Count:14 |
Overview of materials for Polyaryletherketone (PAEK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Carbon Fiber Filled". Each property range of values reported is minimum and .. |
|||
Linear Mold Shrinkage, Transverse | 0.0110 - 0.0190 cm/cm | 0.0110 - 0.0190 in/in | Average value: 0.0162 cm/cm Grade Count:26 |
Overview of materials for Acetal Homopolymer, Unreinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, Unreinforced, Impact Grade". Each property range of values reported is minimum and m.. |
|||
Linear Mold Shrinkage, Transverse | 0.000500 - 0.0190 cm/cm | 0.000500 - 0.0190 in/in | Average value: 0.00923 cm/cm Grade Count:257 |
Overview of materials for Nylon 66, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Linear Mold Shrinkage, Transverse | 0.00100 - 0.0190 cm/cm | 0.00100 - 0.0190 in/in | Average value: 0.0127 cm/cm Grade Count:11 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |