Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.000 - 0.0160 cm/cm | 0.000 - 0.0160 in/in | Average value: 0.00900 cm/cm Grade Count:16 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO) This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO)". Each property range of values reported is minimum and maximum v.. |
|||
Linear Mold Shrinkage, Transverse | 0.00160 - 0.0160 cm/cm | 0.00160 - 0.0160 in/in | Average value: 0.00390 cm/cm Grade Count:7 |
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an.. |
|||
Linear Mold Shrinkage, Transverse | 0.00100 - 0.0160 cm/cm | 0.00100 - 0.0160 in/in | Average value: 0.00953 cm/cm Grade Count:32 |
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |
|||
Linear Mold Shrinkage, Transverse | 0.00600 - 0.0160 cm/cm | 0.00600 - 0.0160 in/in | Average value: 0.00843 cm/cm Grade Count:14 |
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are.. |
|||
Linear Mold Shrinkage, Transverse | 0.00150 - 0.0160 cm/cm | 0.00150 - 0.0160 in/in | Average value: 0.00566 cm/cm Grade Count:137 |
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Linear Mold Shrinkage, Transverse | 0.000400 - 0.0160 cm/cm | 0.000400 - 0.0160 in/in | Average value: 0.0103 cm/cm Grade Count:35 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |
|||
Linear Mold Shrinkage, Transverse | 0.00250 - 0.0160 cm/cm | 0.00250 - 0.0160 in/in | Average value: 0.00810 cm/cm Grade Count:28 |
Overview of materials for Polyetheretherketone, Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Glass Fiber Filled". Each property range of values reported is minimum and maximum.. |