Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00750 - 0.0128 cm/cm | 0.00750 - 0.0128 in/in | Average value: 0.0113 cm/cm Grade Count:3 |
Overview of materials for Polypropylene, Long Glass Fiber 50% This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include.. |