Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | -0.00300 - 0.00900 cm/cm | -0.00300 - 0.00900 in/in | Average value: 0.00457 cm/cm Grade Count:22 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Ether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Ether Grade". Each property range of values reported is minimum a.. |
|||
Linear Mold Shrinkage, Transverse | -0.00200 - 0.00900 cm/cm | -0.00200 - 0.00900 in/in | Average value: 0.00513 cm/cm Grade Count:12 |
Overview of materials for Thermoplastic Polyurethane, Elastomer, Polyester Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane, Elastomer, Polyester Grade". Each property range of values reported is minim.. |
|||
Linear Mold Shrinkage, Transverse | 0.00300 - 0.00900 cm/cm | 0.00300 - 0.00900 in/in | Average value: 0.00673 cm/cm Grade Count:8 |
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35.. |
|||
Linear Mold Shrinkage, Transverse | 0.00750 - 0.00900 cm/cm | 0.00750 - 0.00900 in/in | Average value: 0.00806 cm/cm Grade Count:8 |
Overview of materials for Polycyclohexylenedimethylene Terephthalate (PCT), 30% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT or PCTA, 30% Glass Reinforced".Specific grades with glass content between 25% and 34% are included. .. |
|||
Linear Mold Shrinkage, Transverse | 0.00800 - 0.00900 cm/cm | 0.00800 - 0.00900 in/in | Average value: 0.00867 cm/cm Grade Count:3 |
Overview of materials for PCT, 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PCT, 40% Glass Reinforced". Specific grades with glass content between 35% and 44% are included. Each pr.. |
|||
Linear Mold Shrinkage, Transverse | 0.00400 - 0.00900 cm/cm | 0.00400 - 0.00900 in/in | Average value: 0.00550 cm/cm Grade Count:7 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded". Each property range of values reported is .. |
|||
Linear Mold Shrinkage, Transverse | 0.00400 - 0.00900 cm/cm | 0.00400 - 0.00900 in/in | Average value: 0.00605 cm/cm Grade Count:16 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Linear Mold Shrinkage, Transverse | 0.00200 - 0.00900 cm/cm | 0.00200 - 0.00900 in/in | Average value: 0.00557 cm/cm Grade Count:7 |
Overview of materials for Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 20% Glass Fiber Filled". Specific grades with glass content between 15% an.. |
|||
Linear Mold Shrinkage, Transverse | 0.00100 - 0.00900 cm/cm | 0.00100 - 0.00900 in/in | Average value: 0.00546 cm/cm Grade Count:35 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Linear Mold Shrinkage, Transverse | 0.00800 - 0.00900 cm/cm | 0.00800 - 0.00900 in/in | Average value: 0.00833 cm/cm Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |
|||
Linear Mold Shrinkage, Transverse | 0.00400 - 0.00900 cm/cm | 0.00400 - 0.00900 in/in | Average value: 0.00654 cm/cm Grade Count:13 |
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m.. |
|||
Linear Mold Shrinkage, Transverse | 0.00200 - 0.00900 cm/cm | 0.00200 - 0.00900 in/in | Average value: 0.00544 cm/cm Grade Count:11 |
Overview of materials for Nylon 66/6, 60% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 60% Glass Fiber Reinforced". Specific grades with glass content between 55% and 64% are incl.. |
|||
Linear Mold Shrinkage, Transverse | 0.00100 - 0.00900 cm/cm | 0.00100 - 0.00900 in/in | Average value: 0.00580 cm/cm Grade Count:26 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |
|||
Linear Mold Shrinkage, Transverse | 0.00600 - 0.00900 cm/cm | 0.00600 - 0.00900 in/in | Average value: 0.00817 cm/cm Grade Count:6 |
Overview of materials for Nylon 6-3 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e.. |
|||
Linear Mold Shrinkage, Transverse | 0.00250 - 0.00900 cm/cm | 0.00250 - 0.00900 in/in | Average value: 0.00599 cm/cm Grade Count:4 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |
|||
Linear Mold Shrinkage, Transverse | 0.00250 - 0.00900 cm/cm | 0.00250 - 0.00900 in/in | Average value: 0.00541 cm/cm Grade Count:22 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma.. |
|||
Linear Mold Shrinkage, Transverse | 0.00900 - 0.00900 cm/cm @Temperature 80.0 - 80.0 °C |
0.00900 - 0.00900 in/in @Temperature 176 - 176 °F |
Average value: 0.00900 cm/cm Grade Count:1 |
Overview of materials for Nylon 6, 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. .. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.00900 cm/cm | 0.00500 - 0.00900 in/in | Average value: 0.00770 cm/cm Grade Count:5 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |