Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00200 - 0.00600 cm/cm | 0.00200 - 0.00600 in/in | Average value: 0.00467 cm/cm Grade Count:3 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Linear Mold Shrinkage, Transverse | 0.00200 - 0.00600 cm/cm | 0.00200 - 0.00600 in/in | Average value: 0.00333 cm/cm Grade Count:3 |
Overview of materials for Polystyrene + Polyphenylene Ether, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Unreinforced". Each property range of values reported is minimum and .. |
|||
Linear Mold Shrinkage, Transverse | 0.00250 - 0.00600 cm/cm | 0.00250 - 0.00600 in/in | Average value: 0.00456 cm/cm Grade Count:21 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
Linear Mold Shrinkage, Transverse | 0.00300 - 0.00600 cm/cm | 0.00300 - 0.00600 in/in | Average value: 0.00410 cm/cm Grade Count:15 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Linear Mold Shrinkage, Transverse | 0.00500 - 0.00600 cm/cm | 0.00500 - 0.00600 in/in | Average value: 0.00550 cm/cm Grade Count:4 |
Overview of materials for Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS) Alloy, Glass Reinforced, Flow Enhanced". Each property range of values repor.. |
|||
Linear Mold Shrinkage, Transverse | 0.00600 - 0.00600 cm/cm @Temperature 80.0 - 80.0 °C |
0.00600 - 0.00600 in/in @Temperature 176 - 176 °F |
Average value: 0.00600 cm/cm Grade Count:6 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |
|||
Linear Mold Shrinkage, Transverse | 0.00450 - 0.00600 cm/cm | 0.00450 - 0.00600 in/in | Average value: 0.00528 cm/cm Grade Count:3 |
Overview of materials for Polysulfone, 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polysulfone, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are inc.. |