Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0010 - 0.0020 cm/cm | 0.0010 - 0.0020 in/in | ASTM D955 |
PolyOne Stat-Tech™ PI-05CF/000R Black Polyether Imide (PEI) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Linear Mold Shrinkage, Transverse | 0.00 - 0.0020 cm/cm @Thickness 3.17 mm |
0.00 - 0.0020 in/in @Thickness 0.125 in |
|
Ovation Polymers RIGITRON 30545 GF Polyester, 45% Glass Reinforced Polyester – 45% Glass Fiber Reinforced PET. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to ASTM standards. Var.. |
|||
Linear Mold Shrinkage, Transverse | 0.00 - 0.0020 cm/cm @Thickness 3.20 mm |
0.00 - 0.0020 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 4401R PPC+PC LEXAN 4401R is a high heat resistant poly(ester)carbonate injection molding resin.This data was supplied by SABIC-IP for the Americas region. |
|||
Linear Mold Shrinkage, Transverse | 0.00 - 0.0020 cm/cm @Thickness 3.20 mm |
0.00 - 0.0020 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 4401R PPC+PC (Asia Pacific) LEXAN 4401R is a high heat resistant poly(ester)carbonate injection molding resin.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Linear Mold Shrinkage, Transverse | 0.00 - 0.0020 cm/cm @Thickness 3.20 mm |
0.00 - 0.0020 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 4401R PPC+PC (Europe-Africa-Middle East) LEXAN 4401R is a high heat resistant poly(ester)carbonate injection molding resin.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Linear Mold Shrinkage, Transverse | 0.00 - 0.0020 cm/cm @Thickness 3.20 mm |
0.00 - 0.0020 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 4404 PPC+PC High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi.. |
|||
Linear Mold Shrinkage, Transverse | 0.00 - 0.0020 cm/cm @Thickness 3.20 mm |
0.00 - 0.0020 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 4404 PPC+PC (Asia Pacific) High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi.. |
|||
Linear Mold Shrinkage, Transverse | 0.00 - 0.0020 cm/cm @Thickness 3.20 mm |
0.00 - 0.0020 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® 4404 PPC+PC (Europe-Africa-Middle East) High heat polycarbonate copolymer, with HDT of 287F at 264 psi. FDA food contact compliant. Effective Jan 15th, 2008 this grade should not be used for medical applications which require biocompatibi.. |
|||
Linear Mold Shrinkage, Transverse | 0.00050 - 0.0020 cm/cm @Time 86400 sec |
0.00050 - 0.0020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP DF00A8P PC (Asia Pacific) LNP* Thermocomp* DF00A8P is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good impact perform.. |
|||
Linear Mold Shrinkage, Transverse | 0.00050 - 0.0020 cm/cm @Time 86400 sec |
0.00050 - 0.0020 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP D551 PC (Asia Pacific) LNP* Thermocomp* D551 (or DF00A8P) is a compound based on Polycarbonate resin containing Glass Fiber, Flame Retardant. Added features of this material include: High modulus, good flatness, good impa.. |
|||
Linear Mold Shrinkage, Transverse | 0.0010 - 0.0020 cm/cm @Thickness 3.00 mm |
0.0010 - 0.0020 in/in @Thickness 0.118 in |
|
Unitika UG-100-20 Engineering Plastic Excellent creep resistance, dimensional stability at high temperatureInformation provided by Unitika Ltd. |
|||
Linear Mold Shrinkage, Transverse | 0.00050 - 0.0020 cm/cm | 0.00050 - 0.0020 in/in | ASTM D955 |
PolyOne Stat-Tech™ NJ-20CF/000 Black Polyamide 12 (Nylon 12) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |