Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0156 cm/cm | 0.0156 in/in | |
Plastcom SLOVALEN PC 51 C 20 PP, 20% mineral filling FeaturesModified homopolymer and copolymer PP for injection moulding with the contenct of 20% microground, chemically modified talc. Increased strength, rigidity and thermal application up to 100°C.. |
|||
Linear Mold Shrinkage, Transverse | 0.0156 cm/cm | 0.0156 in/in | STN EN ISO 294-4 |
Plastcom SLOVALEN PC 51 C 40 LS/1M Polypropylene reinforced with mineral filler, UV stabilized Modified copolymer PP for injection molding with the content of 40% mineral filler, UV stabilized. Product meets glow wire test at 750°C. Delivered in full RAL color scale.Information Provided by P.. |
|||
Linear Mold Shrinkage, Transverse | 0.0156 cm/cm | 0.0156 in/in | STN 64 0808 |
Plastcom SLOVALEN PC 51 C 40 Polypropylene Homopolymer and Copolymer, 40% Micronized Talc FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 40% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 120°C... |
|||
Linear Mold Shrinkage, Transverse | 0.0156 cm/cm | 0.0156 in/in | |
Plastcom SLOVALEN PC 51 C 40 PP reinforced with 40% mineral filler Features: Modified homopolymer and copolymer PP for injection moulding with the contenct of 40% microground, chemically modified chalk. Increased strength, rigidity and thermal application up to 100.. |
|||
Linear Mold Shrinkage, Transverse | 0.0156 cm/cm | 0.0156 in/in | |
Plastcom SLOVALEN PC 91 C 20 PP, 20% mineral filling FeaturesModified copolymer PP for injection moulding with the contenct of 20% microground, chemically modified talc. Increased strength, rigidity and thermal application up to 100°C depending on th.. |