Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0135 cm/cm | 0.0135 in/in | STN 64 0808 |
Plastcom SLOVASTER® B GF 15 Polybutylene Terephthalate, 15% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 15% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Linear Mold Shrinkage, Transverse | 0.0135 cm/cm | 0.0135 in/in | LATI |
LATI LATAN 13 G/15 15% Glass Fiber Reinforced Polyoxymethylene Copolymer (POM)
(discontinued **) Description: Latan series thermoplastics are polyoxymethylene copolymer (POM) products. The main applications for Latan feature good wear resistance, chemical inertness and low water absorption (gea.. |
|||
Linear Mold Shrinkage, Transverse | 0.0135 - 0.0165 cm/cm | 0.0135 - 0.0165 in/in | |
LATI Latene® 7H2-V2HF PP Homopolymer, Heat Stabilized, Flame Retardant Polypropylene homopolymer (PPh) based compound. Heat stabilized. UL94 V-2 classified, halogens-based flame retardants free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; No.. |
|||
Linear Mold Shrinkage, Transverse | 0.0135 - 0.0165 cm/cm | 0.0135 - 0.0165 in/in | |
LATI Latene® EP 7-V2HF PP Copolymer, Flame Retardant Polypropylene copolymer (PPc) based compound. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; N.. |
|||
Linear Mold Shrinkage, Transverse | 0.0135 - 0.0165 cm/cm | 0.0135 - 0.0165 in/in | |
LATI Latilub 66-10T Y/15 PA66, 15% Aramid Fiber Reinforced, PTFE Filled Self-lubricating product based on Polyamide 66 (PA66). PTFE. Aramid fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industri.. |
|||
Linear Mold Shrinkage, Transverse | 0.0135 - 0.015 cm/cm | 0.0135 - 0.015 in/in | ISO DIS 294-4 |
Wellman Wellamid® GS1684-WBK1 25% Glass Sphere Filled Nylon 66 Description: Glass Sphere Filled Nylon 66Information provided by Wellman. |
|||
Linear Mold Shrinkage, Transverse | 0.0135 cm/cm | 0.0135 in/in | |
Plastcom SLOVALEN PH 72 T 20 PP, 20% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 20% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc conte nt. Decreased sh.. |