Physical Properties Metric English Comments
Linear Mold Shrinkage, Transverse 0.00900 - 0.0155 cm/cm
0.00900 - 0.0155 in/in
Average value: 0.0127 cm/cm Grade Count:12
Overview of materials for Polyetheretherketone, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value..
Linear Mold Shrinkage, Transverse 0.00900 - 0.0150 cm/cm
0.00900 - 0.0150 in/in
Average value: 0.0135 cm/cm Grade Count:4
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Glass Fiber Filled". Each property range of values reported i..
Linear Mold Shrinkage, Transverse 0.00900 - 0.0300 cm/cm
0.00900 - 0.0300 in/in
Average value: 0.0164 cm/cm Grade Count:11
Overview of materials for Acetal Copolymer, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% ar..
Linear Mold Shrinkage, Transverse 0.00900 - 0.0110 cm/cm
0.00900 - 0.0110 in/in
Average value: 0.00967 cm/cm Grade Count:3
Overview of materials for Nylon 66, 10% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Carbon Fiber Filled". Specific grades with carbon fiber content between 5% and 14% are inc..
Linear Mold Shrinkage, Transverse 0.00900 cm/cm
0.00900 in/in
Average value: 0.00900 cm/cm Grade Count:4
Overview of materials for Nylon 63, 35% Glass-Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 63, 35% Glass-Filled". Each property range of values reported is minimum and maximum values of app..
Linear Mold Shrinkage, Transverse 0.00900 - 0.0170 cm/cm
0.00900 - 0.0170 in/in
Average value: 0.0117 cm/cm Grade Count:4
Overview of materials for Nylon 46, Flame Retarded + Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Flame Retarded + Glass Fiber Reinforced". Each property range of values reported is minimum an..
Linear Mold Shrinkage, Transverse 0.00900 - 0.0210 cm/cm
0.00900 - 0.0210 in/in
Average value: 0.0153 cm/cm Grade Count:8
Overview of materials for Polypropylene Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene Glass Bead Filled". Each property range of values reported is minimum and maximum values o..
Linear Mold Shrinkage, Transverse 0.00900 - 0.00900 cm/cm

@Temperature 80.0 - 80.0 °C
0.00900 - 0.00900 in/in

@Temperature 176 - 176 °F
Average value: 0.00900 cm/cm Grade Count:1
Overview of materials for Nylon 6, 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 10% Glass Fiber Filled". Specific grades with glass content between 5% and 14% are included. ..
Copyright © lookpolymers.com All Rights Reserved