Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00700 - 0.0150 cm/cm | 0.00700 - 0.0150 in/in | Average value: 0.0130 cm/cm Grade Count:4 |
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled". Each property range of values reported .. |
|||
Linear Mold Shrinkage, Transverse | 0.00700 - 0.00800 cm/cm | 0.00700 - 0.00800 in/in | Average value: 0.00780 cm/cm Grade Count:15 |
Overview of materials for Polycarbonate, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Extruded". Each property range of values reported is minimum and maximum values of approp.. |
|||
Linear Mold Shrinkage, Transverse | 0.00700 - 0.0120 cm/cm | 0.00700 - 0.0120 in/in | Average value: 0.00995 cm/cm Grade Count:4 |
Overview of materials for Polypropylene, Mineral Reinforced, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced, Impact Modified". Each property range of values reported is minimum a.. |
|||
Linear Mold Shrinkage, Transverse | 0.00700 - 0.0130 cm/cm | 0.00700 - 0.0130 in/in | Average value: 0.00929 cm/cm Grade Count:14 |
Overview of materials for Nylon 66, Glass Reinforced, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass Reinforced, Impact Grade". Each property range of values reported is minimum and maximum.. |
|||
Linear Mold Shrinkage, Transverse | 0.00700 - 0.0170 cm/cm | 0.00700 - 0.0170 in/in | Average value: 0.0106 cm/cm Grade Count:22 |
Overview of materials for Nylon 612, Glass Fiber Filler This property data is a summary of similar materials in the MatWeb database for the category "Nylon 612, Glass Fiber Filler". Each property range of values reported is minimum and maximum values of .. |
|||
Linear Mold Shrinkage, Transverse | 0.00700 - 0.0120 cm/cm | 0.00700 - 0.0120 in/in | Average value: 0.00888 cm/cm Grade Count:8 |
Overview of materials for Nylon 12, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Linear Mold Shrinkage, Transverse | 0.00700 - 0.0150 cm/cm | 0.00700 - 0.0150 in/in | Average value: 0.0108 cm/cm Grade Count:27 |
Overview of materials for Nylon 46, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values .. |
|||
Linear Mold Shrinkage, Transverse | 0.00700 - 0.0243 cm/cm | 0.00700 - 0.0243 in/in | Average value: 0.0164 cm/cm Grade Count:29 |
Overview of materials for Polypropylene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Flame Retardant". Each property range of values reported is minimum and maximum values of.. |