Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® FXM141R PC (Europe-Africa-Middle East) FXM141R is a Lexan PC grade in Metallic or Pearlescent effect, which is part of the VisualFX family. These effects have been developed to meet increasing Aesthetic demands in the Marketplace. Color .. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm | 0.0050 in/in | Euronil |
Nilit Nilamid A3 H G8 40% Glass Reinforced PA66 Description: Nilamid A3 H G8 is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance, even at elevated temper.. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm | 0.0050 in/in | 415°C nozzle, 200°C tool; ISO 294-4 |
Victrex® PEEK 650CA30 30% Carbon Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, FDA food contact compliant.. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® EXRL0662 PC Med/low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam e-beam and gamma sterilizable. .. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® HP6NR PC (Asia Pacific) Low/med flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains no .. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics Lexan® HPS7 PC Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma sterilizable. .. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm | 0.0050 in/in | Measured on 102 mm X 102 mm X 3.2 mm Plaques, Edge Gated |
Solvay Specialty Polymers Ryton® R-4XT Polyphenylene Sulfide Compound
(Unverified Data**) Natural Color Polyphenylene Sulfide CompoundRyton® R-4XT is a 40% fiberglass reinforced polyphenylene sulfide compound that takes advantage of state-of-the-art polymerization technology to improve .. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm | 0.0050 in/in | 410°C nozzle, 220°C mold |
Gharda Chemicals G-PAEKâ„¢ 1230FC Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic material, 10% carbon fiber, 10% PTFE and 10% graphite reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection mo.. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm | 0.0050 in/in | ISO 294-4 |
Mitsubishi Xantar® MX 1082 Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0075 cm/cm | 0.0050 - 0.0075 in/in | |
LATI Larpeek 10 G/40 PEEK, 40% Glass Fiber Reinforced Polyetheretherketone (PEEK) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle East; As.. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | |
LATI Lastilac 11 G/10 ABS/PC, 10% Glass Fiber Reinforced ABS/PC Blend (ABS/PC) based compound. Glass fibers. Good surface appearance. Good impact resistance. Good thermal properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; .. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0070 cm/cm | 0.0050 - 0.0070 in/in | on Tensile Bar; SABIC Method |
SABIC Innovative Plastics NORYL PX9406 PPE+PS (Asia Pacific) Nonbrominated, nonchlorinated, flame retarded. Improved productivity and reliability. 252F HDT. UL94 V-0 rated. Electrical applications. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics ULTEM 9075 PEI (Asia Pacific) High flow Polyetherimide blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm | 0.0050 in/in | ASTM D955 |
Solvay Specialty Polymers Amodel® A-1565 HS Polyphthalamide (PPA), 65% GlassMineral (Dry) Amodel® A-1565 HS is a 65% glass and mineral-reinforced polyphthalamide (PPA) designed to be cost-effective in applications requiring high stiffness, good dimensional stability and good retention.. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm @Time 86400 sec |
0.0050 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON SE002Z PA 12 (Asia Pacific) LNP* Stat-kon* SE002Z is a compound based on Nylon 12 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0070 cm/cm @Time 86400 sec |
0.0050 - 0.0070 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP AF003 ABS LNP* THERMOCOMP* AF003 is a compound based on ABS resin containing 15% Glass Fiber. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0080 cm/cm | 0.0050 - 0.0080 in/in | ASTM D955 |
Shinkong Synthetic Fibers Shinite® T101G30 PET, 30% Glass Filled Information from Shinkong Synthetic Fibers Corp. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics ULTEM 1000EF PEI (Asia Pacific) Transparent, enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0090 cm/cm | 0.0050 - 0.0090 in/in | DIS 294-4 |
Wellman Wellpet® FRGF116-BK1 Polyethylene Terephthalate, 30% Glass Fiber Reinforced, Flame Retardant All information provided by Wellman Engineered Resins. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm | 0.0050 in/in | |
Chevron Phillips Xtel® XE3035NA Polyphenylene Sulfide Alloy Xtel® XE3035NA is a high performance, glass fiber reinforced, PPS based alloy developed to provide exceptionally high ductility and impact resistance along with good thermal stability.Information p.. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm | 0.0050 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® GTR 45 PA6I/6T Product description: Grivory GTR 45 is a transparent engineering thermoplastic based on amorphous, partially aromatic copolyamide for injection molding. Compared to other semi crystalline polyamides.. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm | 0.0050 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® BGZ-40 PA6-GF40 Product description: Grilon BGZ-40 is a normal viscosity, heat stabilized and impact modified PA 6 injection molding type with 40% glass fibers. Grilon BGZ-40 has the following important properties:.. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm | 0.0050 in/in | ISO 294-4, 2577 |
EMS-Grivory Grivory® HTV-5H1 nat PA6T/6I-GF50 Product description: Grivory HTV-5H1 natural is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Acc. to ISO: PA 6T/6I. Ac.. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics ULTEM 1000EF PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS. US FDA and EU Food Contact compliant. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0070 cm/cm @Thickness 3.20 mm |
0.0050 - 0.0070 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics ULTEM 9076 PEI (Asia Pacific) Standard flow Polyetherimide Blend. Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. ECO Conforming. |
|||
Linear Mold Shrinkage, Transverse | 0.0050 cm/cm | 0.0050 in/in | Sim. To ISO 294-4 |
DSM Novamid® MC112LG55 C10 PA6-GF55 55% Glass Reinforced |
|||
Linear Mold Shrinkage, Transverse | 0.0050 - 0.0070 cm/cm @Time 86400 sec |
0.0050 - 0.0070 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP THERMOCOMP JF002 PES LNP THERMOCOMP* JF002 is a compound based on Polyethersulfone resin containing 10% Glass Fiber. |