Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Transverse | 0.00030 cm/cm @Time 86400 sec |
0.00030 in/in @Time 24.0 hour |
ASTM D955 |
SABIC Innovative Plastics LNP KONDUIT OX11315 PPS (Asia Pacific) Thermally conductive electrically insulative mineral filled PPS FR compound. |
|||
Linear Mold Shrinkage, Transverse | 0.00030 cm/cm | 0.00030 in/in | Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 2577 |
Lanxess Durethan® AKV 40 H2.0 901510 Nylon 66, Glass Fiber Reinforced PA 66, 40% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |