Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 86000 cP @Shear Rate 5000 1/s, Temperature 215 °C |
86000 cP @Shear Rate 5000 1/s, Temperature 419 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers |
|||
Viscosity | 86000 cP @Shear Rate 5000 1/s, Temperature 260 °C |
86000 cP @Shear Rate 5000 1/s, Temperature 500 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 7246 Polyester Elastomer TPC-ET
(Unverified Data**) 72 Shore D High Performance Polyester Elastomer.Information provided by DuPont Performance Polymers |
|||
Viscosity | 86000 cP @Shear Rate 5000 1/s, Temperature 295 °C |
86000 cP @Shear Rate 5000 1/s, Temperature 563 °F |
DAM; ISO 11443 |
DuPont Performance Polymers Zytel® 70G30HSLR NC010 Nylon 66
(Unverified Data**) Zytel® 70G30HSLR NC010 is a 30% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Viscosity | 86000 cP @Shear Rate 5000 1/s, Temperature 295 °C |
86000 cP @Shear Rate 5000 1/s, Temperature 563 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G35HSL NC010 Nylon 66
(Unverified Data**) 35% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G35HSL NC010 is a 35% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform.. |
|||
Viscosity | 86000 cP @Shear Rate 1000 1/s, Temperature 190 °C |
86000 cP @Shear Rate 1000 1/s, Temperature 374 °F |
Apparent Dynamic Viscosity |
Dow DOWLEX™ 2517 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2517 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent environmental stress crack resistance and low temperature properties with excellent f.. |