Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 84000 cP @Shear Rate 5000 1/s, Temperature 230 °C |
84000 cP @Shear Rate 5000 1/s, Temperature 446 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 525GR NC000 Acetal (POM)
(Unverified Data**) 25% Glass Reinforced Medium Viscosity Acetal Homopolymer Delrin 525GR NC000 is a 25% glass reinforced acetal homopolymer for injection molding. It has very high strength stiffness and high deflectio.. |
|||
Viscosity | 84000 cP @Shear Rate 5000 1/s, Temperature 230 °C |
84000 cP @Shear Rate 5000 1/s, Temperature 446 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 527UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized Medium Viscosity Acetal HomopolymerDelrin 527UV NC010 is a medium viscosity acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has improvem.. |