Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 71000 cP @Shear Rate 5000 1/s, Temperature 295 °C |
71000 cP @Shear Rate 5000 1/s, Temperature 563 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 415HP NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 15% Glass Reinforced Polyethylene Terephthalate with Excellent Impact Resistance Rynite 415HP NC010 is a 15% glass reinforced modified polyethylene terephthalate improved for easy fast processing ov.. |
|||
Viscosity | 71000 cP @Shear Rate 5000 1/s, Temperature 295 °C |
71000 cP @Shear Rate 5000 1/s, Temperature 563 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® EFE6053 BK413 Nylon 66
(Unverified Data**) 40% Mineral/Glass Reinforced Polyamide 66 Minlon EFE6053 BK413 is a 40% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance P.. |