Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 327000 cP @Shear Rate 500 1/s, Temperature 210 °C |
327000 cP @Shear Rate 500 1/s, Temperature 410 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4069 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Viscosity | 327000 cP @Shear Rate 500 1/s, Temperature 275 °C |
327000 cP @Shear Rate 500 1/s, Temperature 527 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Rynite® 935 NC010 Polyethylene Terephthalate (PET)
(Unverified Data**) 35% Glass Reinforced Polyethylene Terephthalate Rynite 935 NC010 is a 35% mica/glass reinforced modified polyethylene terephthalate resin with exceptionally low warpage excellent electrical properti.. |